Glaze Material
Percentage
Dolomite 10%
Custer Feldspar 14
Ball Clay 29
EPK Kaolin 38
Silica
9
100%

This recipe is included in 10 Tried and True Raku Glaze Recipes: Recipe Cards for our Favorite Raku Pottery Ceramic Glazes, which is free to Ceramic Arts Daily subscribers.

 