All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
ferro-frit-3214 10.00
Nepheline Syenite 20.00
EPK Kaolin 25.00
OM 4 Ball Clay 25.00
Silica 20.00
Add Amount
borax 5.00
Zircopax 5.00

Instructions

This is my base recipe—it ranges from white to gray to blush depending on the kiln atmosphere. I add approximately 5% additions of stain to create my colored slips. I mix to various thicknesses, sieve it through a 100-mesh screen, and overlap multiple layers to add depth and variation. 

 

This recipe was shared by Heather Lepp in the June/July/August 2025 issue of Ceramics Monthly.