All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 18.18
Wollastonite 20.91
Custer Feldpsar 18.18
Barnard Slip 30.00
Silica 12.73

Instructions

This is a nice glaze for soda and wood. It needs to be applied thinly or it will run.

This recipe was shared by Donovan Palmquist in the March 2025 issue of Ceramics Monthly.