Glaze Material
Percentage
Ferro Frit 3110 80%
EPK Kaolin 20
100%
Add: Bentonite 2%
Blue Variation:
Superpax 15%
Blue stain 10%
Green Variation:
Mint green stain 10%

Stains provide color to the base glaze and superpax is an opacifier that makes the clear base glaze an opaque, glossy white.