A Plethora of Purple: Glaze Recipes for Earthenware, Stoneware and Porcelain
Purple is one of my favorite colors. From pale lavender to deep eggplant there are so many gorgeous purple hues. … Read More
Purple is one of my favorite colors. From pale lavender to deep eggplant there are so many gorgeous purple hues. … Read More
There are a lot of traditional reduction glaze recipes out there, and they are typically formulated for firing at cone … Read More
Glazes in the Chun glaze family are lovely light blue high fire glazes that feature opalescence caused by micro bubbles … Read More
If you are looking to buy a kiln, you will need to consider a kiln exhaust system too. Typically we … Read More
Cobalt blue glaze recipes are in most potters’ repertoires because they produce beautiful blue glazes. And what’s not to love … Read More
Ceramic artists in this day and age have it relatively easy when it comes to obtaining materials for their craft. … Read More
Who can resist a beautiful bright red glaze? But red is also one of the most difficult colors to achieve … Read More
In today’s post, our own Holly Goring not only includes some versatile three-ingredient cone 04 glaze recipes, but she also … Read More
When you pull a piece out of the kiln and there is a glaze defect on it, you might think there … Read More
Years ago, I put a glossy, transparent, gray/off-white glaze into a wood kiln and it came out matte, opaque, and … Read More