How to Make Unique Sterling Silver and Ceramic Earrings Using a Simple Metalworking Technique
Adorn yourself and others with beautiful ceramic jewelry!
Jennifer Allen
I have dabbled a bit in ceramic jewelry making, but have mostly used store bought metal findings and components. But after filming Ceramic
Jewelry Making with ceramic artist Jen Allen and metalsmith Maia Leppo, I became super excited about putting my own touch on the metal components of ceramic jewelry.
In this clip, an excerpt from Ceramic Jewelry Making Part 1, Jen Allen shows how she uses some simple metalworking techniques to create an adorable pair of dangly earrings with a handmade clay bead. Have a look and let your wheels start turning for ways to make this technique your own! – Jennifer Poellot Harnetty, editor
Search the Daily
Published Sep 6, 2024
In this clip, an excerpt from Ceramic Jewelry Making Part 1, Jen Allen shows how she uses some simple metalworking techniques to create an adorable pair of dangly earrings with a handmade clay bead. Have a look and let your wheels start turning for ways to make this technique your own! – Jennifer Poellot Harnetty, editor
This clip was excerpted from Ceramic Jewelry Making, Part One, which is available in the Ceramic Arts Network Shop, or on CLAYflicks!
**First published in 2019.
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques