There is more than one way to make a ceramic coil. Depending on what you are making—coil sculpture or coil pots—the typical round coil may not be the best way to go. Experimenting with flat and triangular coils might save you time and effort in the long run.
In this post, an excerpt from the Ceramics Monthly archive, coil builder Priya Thoresen shares tips on choosing the right ceramic coil for whatever you are building. - Jennifer Poellot Harnetty, editor
Beginning ceramics students often focus on trying to make the most consistently round coils possible. Round coils, however are often not always the most effective shape for building. It may be better to think of the round coil as the basic starting point
that you can expand upon. In this article, I’ll introduce you to the flat coil and the triangle coil.
Flat Coils
To make a flat coil, start with a round coil (1) and flatten it with a paddle or rolling pin (more advanced students could also use the palm of their hand) (2).
• Flat coils add height by making walls taller faster.
• Similar to slabs, flat coils are good at horizontal curves, but less suited to vertical curves.
• Flat coils are good for precise forms and avoiding surface texture.
• If you like to handbuild with a paddle and a Surform, flat coils may be a good choice for you.
Triangle Coils
To make a triangle coil, start with a round coil and pinch or flatten one side of it (3). Considering that a triangle is the strongest shape, it’s no surprise that they have many advantages in handbuilding.
• By stacking triangle coils, it is easier to squish the rows together.
• This also distributes the stress points between the wetter and drier layers, which results in less cracking.
• Triangles inherently have thinner and thicker areas, and can be pinched up, in, or out to add height and shape as you build.
• Building this way will leave texture, and slightly thinner and thicker areas. If you want clean, precise forms, go back to the flat coil.
• Use small triangle coils for filling gaps and reinforcing corners.
Triangle Up or Triangle Down?
Look at what you’re making and think about the shape you’re aiming for or angles you’re joining.
• If you’re going straight up, either way will work.
• For a steep angle outward, attach the triangle at the thinner end, leaving more clay left to stretch outward (4).
• For a steep angle inward, attach the triangle at the thicker end (5).
the author Priya Thoresen received a BA in studio art from Berea College in 2009, and an MFA from Arizona State University in 2017. Thoresen is currently a lecturer at the University of Minnesota and an adjunct faculty member at Concordia University in Saint Paul, Minnesota. To learn more and see Thoresen’s work, visit www.priyathoresen.com.
Search the Daily
Published Aug 9, 2022
There is more than one way to make a ceramic coil. Depending on what you are making—coil sculpture or coil pots—the typical round coil may not be the best way to go. Experimenting with flat and triangular coils might save you time and effort in the long run.
In this post, an excerpt from the Ceramics Monthly archive, coil builder Priya Thoresen shares tips on choosing the right ceramic coil for whatever you are building. - Jennifer Poellot Harnetty, editor
Beginning ceramics students often focus on trying to make the most consistently round coils possible. Round coils, however are often not always the most effective shape for building. It may be better to think of the round coil as the basic starting point that you can expand upon. In this article, I’ll introduce you to the flat coil and the triangle coil.
Flat Coils
To make a flat coil, start with a round coil (1) and flatten it with a paddle or rolling pin (more advanced students could also use the palm of their hand) (2).
• Flat coils add height by making walls taller faster.
• Similar to slabs, flat coils are good at horizontal curves, but less suited to vertical curves.
• Flat coils are good for precise forms and avoiding surface texture.
• If you like to handbuild with a paddle and a Surform, flat coils may be a good choice for you.
Triangle Coils
To make a triangle coil, start with a round coil and pinch or flatten one side of it (3). Considering that a triangle is the strongest shape, it’s no surprise that they have many advantages in handbuilding.
• By stacking triangle coils, it is easier to squish the rows together.
• This also distributes the stress points between the wetter and drier layers, which results in less cracking.
• Triangles inherently have thinner and thicker areas, and can be pinched up, in, or out to add height and shape as you build.
• Building this way will leave texture, and slightly thinner and thicker areas. If you want clean, precise forms, go back to the flat coil.
• Use small triangle coils for filling gaps and reinforcing corners.
Triangle Up or Triangle Down?
Look at what you’re making and think about the shape you’re aiming for or angles you’re joining.
• If you’re going straight up, either way will work.
• For a steep angle outward, attach the triangle at the thinner end, leaving more clay left to stretch outward (4).
• For a steep angle inward, attach the triangle at the thicker end (5).
the author Priya Thoresen received a BA in studio art from Berea College in 2009, and an MFA from Arizona State University in 2017. Thoresen is currently a lecturer at the University of Minnesota and an adjunct faculty member at Concordia University in Saint Paul, Minnesota. To learn more and see Thoresen’s work, visit www.priyathoresen.com.
**First published in 2018.
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques