Nifty Nests: Using Kitchen Gadgets and Textured Slabs to Create Square(ish) Nesting Bowls

Nesting Bowls, by Annie Crietzberg

 

Annie Chrietzberg also loves to scour kitchen stores and garage sales for unique implements to use in the studio. Today, she shares a great little project out of our free download Five Great Handbuilding Techniques: How to Make Pots Using the Pinch, Coil and Slab Methods. Using graduated tart tins with scalloped edges, she demonstrates how to make textured nesting bowls using a simple template system and slab building techniques. – Jennifer Harnetty, editor.


I know I’m not the only overly-involved-with-clay-person out there who brings more things home from a kitchen store for the studio than for the kitchen. So, as I was browsing through a kitchen store, I came across tart tins with scalloped edges and removable bottoms, and knew I’d found something that would be fun and easy to use. I bought four of them in graduated sizes thinking: nesting bowls!

 

To get a square-ish form from a round slab requires removing darts of clay. After experimenting with different dart ratios, I settled on somewhere between a third and a half of the radius. To make the darts template, I traced around the scallops on the cutting edge of the tart tin. Ignoring the low points of the scallops, I cut out a circle and folded it along two perpendicular diameters, so that the folds made a perfect cross. I then found a point somewhere between third and a half way along the radius to cut the darts to. I folded the template in half and cut out a wedge, then used that wedge to cut identical darts all the way around. Explore the possibilities of different sized darts different numbers of darts, and different placement of darts. As long as you keep ratios similar from one template to the next, the bowls should nest.


Learn a plethora of slab techniques from one of the best.
Sandi Pierantozzi shows what can happen when you ask “what if?” in the studio.

Check out her DVD What If? Explorations with Texture and Soft Slabs in the Ceramic Arts Daily Bookstore.


Bevel the darts by pointing the knife point towards the center on each side so you’ll be switching the angle of the knife for each side of the dart. As always with slab work, score, then slip, then score again to create an interface so the seam stays together. You may also want to add a small coil along the seams, since you’re changing the orientation of the slab. Use sponges or small pieces of foam to keep the sides of the bowl just where you want them while you work on the join.

After all four corners are well joined, turn the piece over. Anytime you need to turn a piece over, find foam if needed, and wareboards or bats, and find a way to flip the piece without touching it. Run a finger or a well-wrung-out sponge over the backside of the seam, eliminating any sharpness and sealing it. Repeat these directions with every size tart tin and template that you have, and you will have a lovely little set of nesting bowls. With four nesting bowls, you’ll want to explore the potential using eight different textures-match textures from the top of one bowl to the bottom of the next, let the textures cycle through the set-there are so many possibilities!

 

Tart tins with removable bottoms make excellent studio tools!
  Create a darts template by tracing around the edge. Ignore the scallops when cutting the circle.
  To make sure your bowls nest, use the same dart proportions on each template.
  Clean texture tools before using to avoid getting those little crumbs of clay that can mar the texture, then dust clean texture tools with cornstarch so that they will release.
  Before applying texture, check your slab for size. Leaving an inch or so leeway gives you some room to maneuver if there are flaws in the texture. Smooth the slab with a soft rib.
  Place the slab onto the first texture tool, gently roll from the center towards the edge in a radial pattern, pushing down just enough to press the clay into the texture, but not so hard that you move the clay and thin the slab.
  Flatten the surface with a big rolling pin then carefully place a prepared texture tool on top of the slab and roll using just enough pressure to transfer the texture, but not so much that you thin or move the slab.
  Move to a ware board and remove the texture tools, then flip the slab so the interior face of the bowl is facing up. Use the tart tin to cut through the slab.
  Slip your hand underneath the rim and place your fingertips at the edge of the slab, gently press the slab free of the cutter. Align the darts and then cut the darts with the tip of the knife angled toward the center of the dart on both sides.
  Score and slip the cut edges of darts. Carefully lift slab to join both sides of the dart cuts. Use small foam bolsters to support the sides and keep the corners joined.
  Remove the rough edges with a damp sponge, then lay a small coil in the corner. Blend the coil following the texture, if possible.
Comments
  • Ella M.

    Alice DeLisle April 11, 2012 at 7:15 pm –
    I have tried this and have a high percentage of bowls that warp. Any suggestions on how to prevent warping?

    – May be you use too soft clay? My things are never deformed.

  • Alice D.

    I have tried this and have a high percentage of bowls that warp. Any suggestions on how to prevent warping?

  • Ella M.

    Thank is very creative! Pretty nest.
    Ceramic world is so big! As much as I see others’ artworks in ceramic I want to create all of them! Not to copy but to use some ideas.

  • Salle E.

    GREAT IDEA FOR MY CLAY CLASSES. I USUALLLY GET DOILIES-TEXTURED PIECES FROM RESALE AND “TRASH AND TREASURE” SHOPS. WE RUN THE TEXTURED PIECES ON TOP OF THE WET CLAY THROUGH THE SLAB ROLLER. WORKS GREAT.

  • Annie C.

    I will have ti try that, Lindsay!

  • Lindsay P.

    Love these…remind me of some 40’s and 50’s colorful glass vases! Speaking of ‘nesting’…if you trim a mug/bowl a tad before leather hard…the scraps when gathered and pressed (gently) into a mold or bowl makes a great actual looking nest! It could actually be done in such a way that the ‘nest’ could have enough holes/spaces in it to be used as a sort of collander.

  • Janice W.

    I have also seen this article before but enjoy being reminded of these fantastic projects. Thank you. I will be using this technique when I have my girl friends over for an evening of ‘fun with clay’ as I have some of those tins.

  • On checking my archive I found that this article was earlier posted on July 6, 2009 on Ceramic Arts Daily. It is a welcome reminder. Thanks.

  • This gives me the cue that any thing can be used creatively. Thanks Annie Chrietzberg.

  • Pauline H.

    I will definitely be giving these bowls a go – they are delightful

  • Good Idea using items found in stores.A new Home Depot just opened in our area and will check it out for decorative ideas on my handmade hanging planters.I currently use various stamps I have made from clay and purchased from others for making designs and unusual textures.

  • Annie C.

    The corrugated sheet is a rubber mat that was purchased at Home Depot some years ago.

  • Joy M.

    What is the corrugated sheet you are using?

  • Thanks, this is great. I enjoy browsing, too.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend