Search the Daily

Published Oct 8, 2018

How to Make DIY Texture Rollers with Craft Foam and Wooden Dowels
Every part of the making process involves a decision, and for Catie Miller, choosing a texture is one of the most personal. After working with commercially made texture rollers for a while, she started seeing the same patterns on other potters’ work, and her surfaces began to feel less like her own. She wanted a way to bring her own ideas into her textures.

Catie tried a popular DIY method of drawing with hot glue on a rolling pin, but found the glue hard to control. Since she already used craft foam often in her studio, she tried adhesive-backed foam instead. The result is a roller that’s inexpensive, easy to customize, and has held up well for years. Love this idea! –Jennifer Poellot Harnetty, editor

PS. To see how Catie uses the texture roller, check out her full article in the November/December 2026 issue of Pottery Making Illustrated. Not a subscriber? Subscribe today!

Every part of the making process involves a decision, and choosing a texture is one of the many decisions I make when creating my work. I started thinking more about this after using commercially made texture rollers. I began noticing the same rollers being used by other potters, and the textures I had chosen for my own work started to feel less personal. I wanted a way to customize my textures and incorporate my own ideas into the surface of my work.

I have seen several methods online for making your own texture rollers, including using hot glue on a rolling pin. When I tried this method, I found the hot glue difficult to control. I already use craft foam frequently in my studio, so I wondered if I could use adhesive-backed foam to create a roller instead. After some experimenting, I found a method that was inexpensive, easy to customize, and has held up surprisingly well over the years.

Gathering Supplies (1)

  • 2-mm adhesive-backed craft foam 
  • 1¼-in. × 48-in. round wood dowel 
  • Scissors
  • Ballpoint pen
  • Saw (optional)

The wooden dowels I use are available at most home-improvement stores for around $6 each. I typically cut each 48-inch (1.2 m) dowel into three 16-inch (40.6 cm) rollers, but you can make them as long or short as you want. The length of the roller can also become part of the design depending on the size of the slabs you typically work with.

I originally experimented with PVC pipe because I had some available in my studio. While it worked, I found that clay tended to stick to the plastic more than it does to the wood. 

1 Supplies: adhesive-backed craft foam, a wooden dowel, and scissors. 2 Cut your shapes, then use a ballpoint pen to impress marks into the foam.

Making the Roller

Start by cutting your wooden dowel to your desired length. I usually make mine about 16 inches (40.6 cm) long because of the size of my large platters. Then, cut shapes from the adhesive-backed craft foam and arrange them around the dowel. Once you are happy with the arrangement, peel off the backing and press the foam firmly onto the dowel.

I typically cut my shapes by hand with scissors. I like that this keeps the process simple and low-tech. If you want to create more precise or complicated shapes, a vinyl cutting machine such as a Silhouette or Cricut can also cut craft foam.

One of my favorite things about working with the foam is that the surface can be altered before it ever touches the clay. A ballpoint pen can be used to impress lines, dots, or other details directly into the foam (2). These marks create a softer, subtler impression in the clay than the edges of the cut foam do. You can also experiment with different spacing, orientations, and repetitions. I have not experimented with layering the foam, but I imagine there are plenty of possibilities there.

Once the shapes are cut and detailed, remove the adhesive backing and adhere the shapes directly to the wooden dowel (3). 

3 Peel off the craft foam backing and press the foam onto the dowel.

Catie Miller is a ceramic artist based in Fargo, North Dakota, where she makes pots featuring her brightly illustrated surfaces. For more about her work, visit catie-miller.com. 

Unfamiliar with any terms in this article? Browse our glossary of pottery terms!