Making handmade ceramic planters has become one of my favorite things to do in the studio in the past couple years as my obsession with houseplants has grown (currently wishing I could add on to my house because I am out of sunny windows!). So I am always excited to see how other artists approach the handmade planter form.
In this post, an excerpt from the Pottery Making Illustrated archive, Erika Novak shares how to make a clay planter on the pottery wheel. I love how Erika takes advantage of the fact that these are hanging planters and creates lovely detail at the bottom. –Jennifer Poellot Harnetty, editor
I found my love for surface design in clay early on in my ceramics journey. The evolution of my work started with simple carvings on thrown forms and became more complex and decorative over the years. I love bright color combinations contrasted against
a raw clay body. I also have a fondness for functional pieces. In the development of my hanging planters, I played with the idea of giving function to a hanging sculptural object. I also love the addition of the natural texture of a live plant cascading
down the side of the pot. To me, the plant complements the planter just as a latte can complement the cup. Many of my planters are a round form with a decorative, elongated point, which was inspired by a trip out west. While browsing in an iron shop,
I fell in love with a display of various hanging mosaic lamps with ornamental iron points. In the early stages of figuring out this form, I found it best to throw them upside down as a closed form where I could pull up a little point from the top
of an orb.
Throwing a Hanging Clay Planter
Start with a 2–5 pound (0.9–2.3 kg) ball of clay, wedged and ready to throw. Over the years I have used a few different speckled buff, brown, and porcelain clay bodies made by Laguna.
Once centered, open the clay as wide as you want the opening of the planter to be. Open down to the bat not to waste clay. Because these pots are thrown upside down they won’t need a base (1). For the first pull, I go for a volcano shape, keeping
the base wide and tapering the walls in as I pull higher. On the next pull, begin to round out the belly of the form, but keep the rim tight in and under control. Next, collar in the shoulder and rim of the pot. The goal is to close this form up into
an orb, so make sure to leave extra clay at the rim. You want the top third of the pot on the thicker side so you don’t run out of clay before the form is fully closed (2).
Sometimes when aggressively collaring in, the rim can become off-center. Trim it off with a needle tool before it gets too out of hand. The pot must be as centered as possible to close it and pull a little point. I keep the belly of the pot round while
continuing to close the form. To do this, collar and pull at the same time. Hold the clay steady and collar with one hand while pinching to pull up higher with the other (3). Then, with the extra clay, pinch the form closed completely. You should
be left with a little nub of clay at the top (4). You can pull this nub slightly higher if you want a longer point.
Now that the clay is closed up you essentially have a big air bubble. The air trapped inside will support the clay so you can press on it with more force than you would an open vessel. This is your opportunity to refine the form. Using a flexible steel
rib round and smooth out the surface of the pot (5). I use a steel rib to smooth the surface of every piece I throw. I like to remove all the slip and water from the outside of the piece so the surface is as smooth as possible. Once you are satisfied
with the pot’s shape and surface, carefully cut it from the bat. Make sure not to warp the walls. Remember, it has no base holding the walls in place like a vase would. I use a needle tool while spinning the wheel to cut off rather than a wire
tool to avoid warping (6).
Before you wrap up your pot, dry poke a little air hole with the needle tool in the closed form to release the air. Sometimes the pot will suction back to the bat after cutting it, and with nowhere to go, the compressed air can cause a split in the top
of the closed form, especially if you have thrown thin walls. To prevent this from happening, I will poke an air hole to be safe.
Trimming the Clay Planter
To trim, first, throw a chuck for the pot to sit upside down in. Make sure the chuck is on center and thick enough to support the piece. Remove all the slip from the outside of the chuck with a steel rib. This will prevent your piece from getting stuck
to the chuck (7). After centering the piece in the chuck, use a needle tool to further trim out the thicker edge of the base so the walls at the opening are even (8). Remove any extra clay (9). This is now the top of the planter so take time to refine
it by trimming and rounding the rim.
Next, flip and recenter the planter on the wheel so the point is right side up. Using a small trimming tool, trim and refine the shape of the point (10). Making this little ornate detail can be very fun. It is also stressful. Take your time and go slow
to avoid snapping off the point.
Erika Novak lives and works in Connecticut. She began her career as a full-time potter directly after graduating from Central Connecticut State University with a BA in ceramics and geography. She and her partner, Drew Darley, work side by side in their studio, Round Trip Clayworks, at The Farmington Valley Art Center in Avon. Erika is the head of the vibrant art center’s ceramics program where both she and Drew teach classes and run workshops for their community. To see more of her work, visit www.roundtripclayworks.comor www.artsfvac.org/ceramics-programand follow her on Instagram @roundtripclayworks.
Search the Daily
Published Sep 3, 2025
Making handmade ceramic planters has become one of my favorite things to do in the studio in the past couple years as my obsession with houseplants has grown (currently wishing I could add on to my house because I am out of sunny windows!). So I am always excited to see how other artists approach the handmade planter form.
In this post, an excerpt from the Pottery Making Illustrated archive, Erika Novak shares how to make a clay planter on the pottery wheel. I love how Erika takes advantage of the fact that these are hanging planters and creates lovely detail at the bottom. –Jennifer Poellot Harnetty, editor
PS. To find out how Erika creates her lovely surface decoration, check out her article in the May/June 2024 issue of Pottery Making Illustrated! Not a subscriber? Subscribe here!
I found my love for surface design in clay early on in my ceramics journey. The evolution of my work started with simple carvings on thrown forms and became more complex and decorative over the years. I love bright color combinations contrasted against a raw clay body. I also have a fondness for functional pieces. In the development of my hanging planters, I played with the idea of giving function to a hanging sculptural object. I also love the addition of the natural texture of a live plant cascading down the side of the pot. To me, the plant complements the planter just as a latte can complement the cup. Many of my planters are a round form with a decorative, elongated point, which was inspired by a trip out west. While browsing in an iron shop, I fell in love with a display of various hanging mosaic lamps with ornamental iron points. In the early stages of figuring out this form, I found it best to throw them upside down as a closed form where I could pull up a little point from the top of an orb.
Throwing a Hanging Clay Planter
Start with a 2–5 pound (0.9–2.3 kg) ball of clay, wedged and ready to throw. Over the years I have used a few different speckled buff, brown, and porcelain clay bodies made by Laguna.
Once centered, open the clay as wide as you want the opening of the planter to be. Open down to the bat not to waste clay. Because these pots are thrown upside down they won’t need a base (1). For the first pull, I go for a volcano shape, keeping the base wide and tapering the walls in as I pull higher. On the next pull, begin to round out the belly of the form, but keep the rim tight in and under control. Next, collar in the shoulder and rim of the pot. The goal is to close this form up into an orb, so make sure to leave extra clay at the rim. You want the top third of the pot on the thicker side so you don’t run out of clay before the form is fully closed (2).
Sometimes when aggressively collaring in, the rim can become off-center. Trim it off with a needle tool before it gets too out of hand. The pot must be as centered as possible to close it and pull a little point. I keep the belly of the pot round while continuing to close the form. To do this, collar and pull at the same time. Hold the clay steady and collar with one hand while pinching to pull up higher with the other (3). Then, with the extra clay, pinch the form closed completely. You should be left with a little nub of clay at the top (4). You can pull this nub slightly higher if you want a longer point.
Now that the clay is closed up you essentially have a big air bubble. The air trapped inside will support the clay so you can press on it with more force than you would an open vessel. This is your opportunity to refine the form. Using a flexible steel rib round and smooth out the surface of the pot (5). I use a steel rib to smooth the surface of every piece I throw. I like to remove all the slip and water from the outside of the piece so the surface is as smooth as possible. Once you are satisfied with the pot’s shape and surface, carefully cut it from the bat. Make sure not to warp the walls. Remember, it has no base holding the walls in place like a vase would. I use a needle tool while spinning the wheel to cut off rather than a wire tool to avoid warping (6).
Before you wrap up your pot, dry poke a little air hole with the needle tool in the closed form to release the air. Sometimes the pot will suction back to the bat after cutting it, and with nowhere to go, the compressed air can cause a split in the top of the closed form, especially if you have thrown thin walls. To prevent this from happening, I will poke an air hole to be safe.
Trimming the Clay Planter
To trim, first, throw a chuck for the pot to sit upside down in. Make sure the chuck is on center and thick enough to support the piece. Remove all the slip from the outside of the chuck with a steel rib. This will prevent your piece from getting stuck to the chuck (7). After centering the piece in the chuck, use a needle tool to further trim out the thicker edge of the base so the walls at the opening are even (8). Remove any extra clay (9). This is now the top of the planter so take time to refine it by trimming and rounding the rim.
Next, flip and recenter the planter on the wheel so the point is right side up. Using a small trimming tool, trim and refine the shape of the point (10). Making this little ornate detail can be very fun. It is also stressful. Take your time and go slow to avoid snapping off the point.
Erika Novak lives and works in Connecticut. She began her career as a full-time potter directly after graduating from Central Connecticut State University with a BA in ceramics and geography. She and her partner, Drew Darley, work side by side in their studio, Round Trip Clayworks, at The Farmington Valley Art Center in Avon. Erika is the head of the vibrant art center’s ceramics program where both she and Drew teach classes and run workshops for their community. To see more of her work, visit www.roundtripclayworks.com or www.artsfvac.org/ceramics-program and follow her on Instagram @roundtripclayworks.
**First published in 2024.
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques