Making impressions in clay is a ton of fun. Making your own stamps makes it even more fun because it allows you to really personalize your work. There are a wide variety of ways to make stamps, and today I am sharing one I thought was pretty nifty
In this post, an excerpt from his book From a Slab of Clay, Daryl Baird shows us how to make our own stamps or press molds using a great transfer technique and insulating foam. Daryl also shows us how he uses his stamp as a press mold to make tiles. –Jennifer Poellot Harnetty, editor
There it is, in front of you—a freshly rolled slab of clay. It’s about 3/8 inch thick and 15 inches in diameter. In this pristine state it’s almost like a blank canvas. And in the same way a novice painter may find the blank canvas a
little intimidating, you may find yourself looking at the slab of clay and wondering where to start, wondering what to do with it.
Simple as it may seem, tile making is the perfect way to begin working with slabs of clay. It helps familiarize you with your clay and with the essential tools used in most slab work including: slab boards, a rolling pin or slab roller, measuring, cutting
and decorating tools.
Before getting started, make a few prototypes where you can master the techniques and discover the textures that will increase the likelihood your projects will come out of the kiln just the way you want.
Carving Your Press Mold
Tools and Materials
Charcoal stick
a soft lead pencil with eraser
paper
indelible marker
a block of foam insulation
Dremel-type rotary tool
X-Acto knife with No. 11 blade
small roller, straightedge
needle tool or cutting knife
Slabs of fresh soft clay are perfect for pressing designs into. Here’s an easy-to-make foam mold with limitless design and texture possibilities.
Search the Daily
Published Oct 28, 2020
In this post, an excerpt from his book From a Slab of Clay, Daryl Baird shows us how to make our own stamps or press molds using a great transfer technique and insulating foam. Daryl also shows us how he uses his stamp as a press mold to make tiles. –Jennifer Poellot Harnetty, editor
There it is, in front of you—a freshly rolled slab of clay. It’s about 3/8 inch thick and 15 inches in diameter. In this pristine state it’s almost like a blank canvas. And in the same way a novice painter may find the blank canvas a little intimidating, you may find yourself looking at the slab of clay and wondering where to start, wondering what to do with it.
Simple as it may seem, tile making is the perfect way to begin working with slabs of clay. It helps familiarize you with your clay and with the essential tools used in most slab work including: slab boards, a rolling pin or slab roller, measuring, cutting and decorating tools.
Before getting started, make a few prototypes where you can master the techniques and discover the textures that will increase the likelihood your projects will come out of the kiln just the way you want.
Carving Your Press Mold
Tools and MaterialsSlabs of fresh soft clay are perfect for pressing designs into. Here’s an easy-to-make foam mold with limitless design and texture possibilities.
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques