In this post, Lisa Naples shares her technique for making a slab-built handle for a cream pitcher. I love this handle because it is an interesting shape that complements her slab-built pitcher really well, and because, just by looking at it, you can tell it is comfortable.
Search the Daily
Published Mar 24, 2023
In this post, Lisa Naples shares her technique for making a slab-built handle for a cream pitcher. I love this handle because it is an interesting shape that complements her slab-built pitcher really well, and because, just by looking at it, you can tell it is comfortable.
Have a look in this excerpt from Flat to Functional: Slab Building and Slip Decorating! —Jennifer Poellot Harnetty, editor
To learn more about Lisa Naples or to see more images of her work, please visit www.lisanaples.com.
**First published in 2014.
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques