A Super Smart Way to Remove Excess Slip When Doing Mishima Slip Inlay
Julia Galloway explains how to make short work of cleaning off excess slip when doing the mishima technique!
Julia Galloway
I have seen lots of ways to remove excess slip when doing Mishima slip inlay or other slip-inlay techniques, from scraping it off with a metal rib to wiping with a damp sponge. But I must say Julia Galloway’s method made me gasp! Julia simply runs her pots under water and wipes away the slip. I figured running a leather-hard pot under water would result in weakening or cracks, but as Julia explains, if the pot is hard leather hard, it can take it.
Using Julia's Mishima slip inlay method has the potential to save lots of time in the wiping-off process. It is also just super satisfying to watch! Have a look at this demo of the process, excerpted from her videoElevating the Handmade and see if it makes you gasp! - Jennifer Poellot Harnetty, editor
Remove Slip Quickly and Easily with Julia Galloway’s Technique
Be aware that Julia plugs up her sink so as not to let the slip go down the drain. Then she lets the water evaporate some, and scoops out the goopy slip and reuses it.
Mishima Definition: East Asian method of creating an inlaid effect by applying contrasting slip into a design incised in leather-hard clay. When the slip stiffens, the excess is scraped off (unless, of course, you try Julia's method!). Source: Clay: A Studio Handbook
See this post for another great way to simplify the clean up process with mishima slip inlay using wax resist. Chandra DeBuse swears by this method to give her great results, and simplify her process.
Search the Daily
Published Jun 20, 2025
I have seen lots of ways to remove excess slip when doing Mishima slip inlay or other slip-inlay techniques, from scraping it off with a metal rib to wiping with a damp sponge. But I must say Julia Galloway’s method made me gasp! Julia simply runs her pots under water and wipes away the slip. I figured running a leather-hard pot under water would result in weakening or cracks, but as Julia explains, if the pot is hard leather hard, it can take it.
Using Julia's Mishima slip inlay method has the potential to save lots of time in the wiping-off process. It is also just super satisfying to watch! Have a look at this demo of the process, excerpted from her video Elevating the Handmade and see if it makes you gasp! - Jennifer Poellot Harnetty, editor
Remove Slip Quickly and Easily with Julia Galloway’s Technique
This clip was excerpted from Elevating the Handmade: Creating Pottery with Personal Meaning, which is available in the Ceramic Arts Network Shop!
Save your pipes and protect the environment!
Be aware that Julia plugs up her sink so as not to let the slip go down the drain. Then she lets the water evaporate some, and scoops out the goopy slip and reuses it.
Mishima Definition: East Asian method of creating an inlaid effect by applying contrasting slip into a design incised in leather-hard clay. When the slip stiffens, the excess is scraped off (unless, of course, you try Julia's method!). Source: Clay: A Studio Handbook
See this post for another great way to simplify the clean up process with mishima slip inlay using wax resist. Chandra DeBuse swears by this method to give her great results, and simplify her process.
**First published in 2016.
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques