Here is an easy way to make a scoring tool with only three materials: a wooden craft stick, toothpicks, and a length of sticky tape. Not only is it cheap to make, so you can make one for every tool stash, but it is also kid friendly as it is not sharp. 

To create this tool, begin by cutting a 5-inch (15-cm) length of sticky tape and keep it close by. Then, place five bamboo toothpicks on top of a wooden craft stick (1). The pointy ends of the toothpicks should overhang the wooden craft stick by about ¼ inch (5 mm). Make sure to lightly tap the ends onto a flat surface to ensure the tips have the same height (2).

1 Place five bamboo toothpicks on top of a wooden craft stick. 2 Make sure to lightly tap the ends onto a flat surface to ensure the tips have the same height. 

Next, hold the stick securely while neatly wrapping the tape around the toothpicks and wooden craft stick so they hold together firmly (3). You are now ready to score and join clay (4). These are great if you run workshops where tools may get lost or damaged, as they are easily and cheaply replaced. 

3 Hold the stick securely while neatly wrapping the tape around the toothpicks and wooden craft stick so they hold together firmly.

4 You are now ready to score and join clay.

See more of Phi Morton’s work on Instagram @phi_morton_art. 

 

Previous October Issue Article                    Next October Issue Article

 

October 2025: Table of Contents


Must-Reads from Ceramics Monthly

Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Click the cover image to return to the Table of Contents