Handbuilding is an ancient pottery-making technique that involves creating forms without a pottery wheel, using the hands, fingers, and simple tools. The most common handbuilding techniques are pinch pottery, coil building, and slab building.

To make a pinch pot, one inserts a thumb into a ball of clay and continually pinches the the clay between the thumb and fingers while rotating to thin out and raise the height of the vessel. Pinching can deliver a pleasingly organic look, but can also yield beautiful, refined results.