A Slick Way to Transfer Printed Designs onto Curved Surfaces
Here’s a process suitable for bisque-fired pots that yields graphic imagery!
Shawna Pincus
Surface design techniques are endless but often favor application on flat planes. Since many ceramic surfaces are not flat, potters have come up with clever ways to transfer screen-printed designs to their work.
Today's post is another example of this ingenuity. In this excerpt from theCeramics Monthly archive, Shawna Pincus explains how she uses a tool used in printmaking to transfer screen-printed imagery to her pots. - Jennifer Poellot Harnetty, editor
Gelli printing plates are readily available at local craft stores, or online. They come in a variety of sizes, so find the size that works best for you and your work. I tend to use smaller 4-inch circles to print on small items, 5-inch squares for singular
or vignetted images, and an 8×10-inch rectangle for larger, continuous designs. Creating a screen with artwork is its own process. There are many screen-printing kits you can buy through a variety of online and physical stores (see the
Resources list at the end of this article). Screens are pretty simple to expose, easy to store, and fairly inexpensive.
Since traditional printmaking ink won’t stand up to the kiln’s temperatures, a ceramic pigment must be used. Commercial underglazes come in a variety of colors and work well with the screens. Underglazes will need to be thickened before using
them with this process. This can be achieved by simply leaving the jar lid open for a few days, and stirring occasionally, until a sour cream–like consistency is reached. I find that different brands of underglaze, and even different colors
within the same brand, need to be slightly different consistencies in order to print properly, so some experimentation is needed.
Method
To give a little extra cushion before printing, place the Gelli printing plate onto a sheet of thin craft foam. Lay a screen face up on the printing plate, keeping in mind that your image will be transferred in reverse (make sure to consider this when
designing your image, especially if you are incorporating text). Apply a small amount of thickened underglaze to a squeegee or flat rubber rib (1), then, holding the screen with one hand, drag the squeegee across the screen at a 45° angle, making
sure to evenly distribute the underglaze over your image (2). Lift the squeegee and drag it across the image again, angling the squeegee up a bit more to collect the excess underglaze. You may need to repeat these steps to completely cover the image
with an even layer of underglaze.
Lift the screen from the Gelli printing plate (3). Working quickly so the underglaze doesn’t dry out, gently roll your pottery over the image on the printing plate (4). The dry ceramic surface will absorb the underglaze, immediately transferring
the print from the printing plate to your clay. To print on a flat surface or interior, pick the printing plate up and gently press it onto the surface of your piece. Once you have completed a print, clean up the Gelli printing plate with a damp
sponge, dry it off, and repeat the process. The screen can also be cleaned with a damp sponge; however, there is no need to clean it between prints unless the underglaze starts to dry and clog the screen.
the author Shawna Pincus is a ceramic artist living in Baltimore, Maryland, with her husband, daughter, and their very fluffy cat. She grew up near Philadelphia, Pennsylvania, and attended the Maryland Institute College of Art in Baltimore, Maryland. She currently works full time in her studio in addition to teaching pottery classes at Baltimore Clayworks as well as through various online workshops. You can find more information on her process and artwork at www.pinkkisspottery.comor @pinkkisspottery on Instagram.
Search the Daily
Published Nov 4, 2024
Today's post is another example of this ingenuity. In this excerpt from the Ceramics Monthly archive, Shawna Pincus explains how she uses a tool used in printmaking to transfer screen-printed imagery to her pots. - Jennifer Poellot Harnetty, editor
PS. For Shawna's helpful troubleshooting tips, check out the May 2022 issue of Ceramics Monthly.
Preparing to Print
Gelli printing plates are readily available at local craft stores, or online. They come in a variety of sizes, so find the size that works best for you and your work. I tend to use smaller 4-inch circles to print on small items, 5-inch squares for singular or vignetted images, and an 8×10-inch rectangle for larger, continuous designs. Creating a screen with artwork is its own process. There are many screen-printing kits you can buy through a variety of online and physical stores (see the Resources list at the end of this article). Screens are pretty simple to expose, easy to store, and fairly inexpensive.
Since traditional printmaking ink won’t stand up to the kiln’s temperatures, a ceramic pigment must be used. Commercial underglazes come in a variety of colors and work well with the screens. Underglazes will need to be thickened before using them with this process. This can be achieved by simply leaving the jar lid open for a few days, and stirring occasionally, until a sour cream–like consistency is reached. I find that different brands of underglaze, and even different colors within the same brand, need to be slightly different consistencies in order to print properly, so some experimentation is needed.
Method
To give a little extra cushion before printing, place the Gelli printing plate onto a sheet of thin craft foam. Lay a screen face up on the printing plate, keeping in mind that your image will be transferred in reverse (make sure to consider this when designing your image, especially if you are incorporating text). Apply a small amount of thickened underglaze to a squeegee or flat rubber rib (1), then, holding the screen with one hand, drag the squeegee across the screen at a 45° angle, making sure to evenly distribute the underglaze over your image (2). Lift the squeegee and drag it across the image again, angling the squeegee up a bit more to collect the excess underglaze. You may need to repeat these steps to completely cover the image with an even layer of underglaze.
Lift the screen from the Gelli printing plate (3). Working quickly so the underglaze doesn’t dry out, gently roll your pottery over the image on the printing plate (4). The dry ceramic surface will absorb the underglaze, immediately transferring the print from the printing plate to your clay. To print on a flat surface or interior, pick the printing plate up and gently press it onto the surface of your piece. Once you have completed a print, clean up the Gelli printing plate with a damp sponge, dry it off, and repeat the process. The screen can also be cleaned with a damp sponge; however, there is no need to clean it between prints unless the underglaze starts to dry and clog the screen.
Resources:
Gelli Printing Plates
www.gelliarts.com
Silkscreens
www.ezscreenprint.com
www.maycocolors.com/creative-tools/designer-silkscreens
www.speedballart.com/speed-screens
the author Shawna Pincus is a ceramic artist living in Baltimore, Maryland, with her husband, daughter, and their very fluffy cat. She grew up near Philadelphia, Pennsylvania, and attended the Maryland Institute College of Art in Baltimore, Maryland. She currently works full time in her studio in addition to teaching pottery classes at Baltimore Clayworks as well as through various online workshops. You can find more information on her process and artwork at www.pinkkisspottery.com or @pinkkisspottery on Instagram.
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques