If you’re a potter and you love making loose leaf tea, making a ceramic tea infuser is a project you will certainly want to take on at some point.
In Gwendolyn Yoppolo’s video,Making a Thrown and Handbuilt Tea Infuser Set, she shares how to make a tea infuser set that includes a mug, strainer, and strainer rest. In this clip, an excerpt from her video, Gwendolyn give tips for getting the tea strainer holes just right, including when to drill them, how thick the walls should be, and how to fix mistakes! –Jennifer Poellot Harnetty, editor
Search the Daily
Published Sep 29, 2023
If you’re a potter and you love making loose leaf tea, making a ceramic tea infuser is a project you will certainly want to take on at some point.
In Gwendolyn Yoppolo’s video, Making a Thrown and Handbuilt Tea Infuser Set, she shares how to make a tea infuser set that includes a mug, strainer, and strainer rest. In this clip, an excerpt from her video, Gwendolyn give tips for getting the tea strainer holes just right, including when to drill them, how thick the walls should be, and how to fix mistakes! –Jennifer Poellot Harnetty, editor
CLAYflicks subscribers can view this and all of CAN's full-length videos on CLAYflicks! Not a subscriber yet? No problem—click here to sign up.
**First published in 2020.
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques