Today's video clip didn't quite fit onto Meredith Host's video because we ran out of space. But I just couldn't bear having it languish on the cutting room floor, so I decided to share it with you all today.
As we all know, transferring two-dimensional designs onto a three-dimensional surface can be challenging - especially if that surface is curvy. In this clip, Meredith shows how she approaches screen printed and stenciled decoration on one of her curvy mugs. - Jennifer Poellot Harnetty, editor
Search the Daily
Published Feb 18, 2022
As we all know, transferring two-dimensional designs onto a three-dimensional surface can be challenging - especially if that surface is curvy. In this clip, Meredith shows how she approaches screen printed and stenciled decoration on one of her curvy mugs. - Jennifer Poellot Harnetty, editor
This clip was excerpted from Form, Pattern, and Underglaze: Wheel Throwing and Decorating, which is available in the Ceramic Arts Network Shop!
To learn more about Meredith Host or to see more images of her work, please visit www.meredithhost.com.
**First published in 2014.
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques