Dipping pots in glaze can be challenging at times—especially when you can't hold onto a foot ring. Glazing tongs can leave unpleasant marks on the glaze surface and require some clean up.
While browsing theCeramics Monthly archive,I stumbled upon Joe Thompson's genius glaze-dipping hack: the car dent puller! Joe uses the small suction device to hold onto his pots while glazing. Simply brilliant! –Jennifer Poellot Harnetty, editor
There are many situations where you want to dip a piece in slip or glaze without using tongs or your fingers to keep hold of
it including greenware being glazed for a single firing, a piece that’s too wide or awkward to safely grip, or pieces that you don’t want to have tong or finger marks in the glaze.
My glaze dipping solution is to use a car dent puller. They’re small suction devices designed to, as the name indicates, pull dents out of car bodywork. The good news for ceramic artists is that they have a comfortable handle attached to a powerful
suction cup, and they’re well suited to gripping pots. I use the smallest one I could find, which is 2½ inches (6 cm) in diameter, and have tested it holding pots that weigh up to 11 pounds (5 kg). As long as the seal is good, it should
be able to comfortably hold most pieces.
To use the dent puller when glazing, make sure the bottom of your piece is relatively smooth and apply wax resist
to a flat area a little bigger than your dent puller. The wax resist is important as the puller can’t create suction on the porous clay surface. Add a little water to the suction cup and position the puller centrally on the piece, then press
it firmly down and move the lever to attach (1). Check that it is securely attached, then dip as normal (2). Remove the dent puller when the piece is dry enough to handle without disturbing the glaze.
Search the Daily
Published Jul 9, 2024
Dipping pots in glaze can be challenging at times—especially when you can't hold onto a foot ring. Glazing tongs can leave unpleasant marks on the glaze surface and require some clean up.
While browsing the Ceramics Monthly archive, I stumbled upon Joe Thompson's genius glaze-dipping hack: the car dent puller! Joe uses the small suction device to hold onto his pots while glazing. Simply brilliant! –Jennifer Poellot Harnetty, editor
My glaze dipping solution is to use a car dent puller. They’re small suction devices designed to, as the name indicates, pull dents out of car bodywork. The good news for ceramic artists is that they have a comfortable handle attached to a powerful suction cup, and they’re well suited to gripping pots. I use the smallest one I could find, which is 2½ inches (6 cm) in diameter, and have tested it holding pots that weigh up to 11 pounds (5 kg). As long as the seal is good, it should be able to comfortably hold most pieces.
**First published in 2020.
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques