Kyla Toomey has come up with a super smart way to make ceramic buttons. By creating a simple press mold with readily available clay tools, Kyla makes it simple to crank out a bunch of clay buttons in one sitting. In fact, it’s so simple to make these ceramic buttons, she can do it while catching up on her favorite movies and shows. Genius.
In this excerpt from her video Uncommon Impressions: Making Your Mark with Handmade Tools, Kyla shares how to make ceramic buttons, and how to use them to embellish her ice cream bowls. I was surprised that you can put these bone-dry clay buttons right onto freshly thrown pots and not worry about them popping off. Who knew? And I love the pop of color the underglaze gives the finished bowls!
Have a look and then have fun thinking of ways to embellish your pots! –Jennifer Poellot Harnetty, editor
Search the Daily
Published Nov 1, 2024
Kyla Toomey has come up with a super smart way to make ceramic buttons. By creating a simple press mold with readily available clay tools, Kyla makes it simple to crank out a bunch of clay buttons in one sitting. In fact, it’s so simple to make these ceramic buttons, she can do it while catching up on her favorite movies and shows. Genius.
In this excerpt from her video Uncommon Impressions: Making Your Mark with Handmade Tools, Kyla shares how to make ceramic buttons, and how to use them to embellish her ice cream bowls. I was surprised that you can put these bone-dry clay buttons right onto freshly thrown pots and not worry about them popping off. Who knew? And I love the pop of color the underglaze gives the finished bowls!
Have a look and then have fun thinking of ways to embellish your pots! –Jennifer Poellot Harnetty, editor
PS. Check out this post in the CAD archives for more ideas on making texture tools for clay! PSS. Check out the Daily archive for ideas on making ceramic jewelry!
This clip was excerpted from Uncommon Impressions with Kyla Toomey, which is available in the Ceramic Arts Network Shop.
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques