Lisa Bare Culp demonstrates a similar technique to Mark’s stamped rim technique, but on a simple vase form. I think it can valuable to see similar techniques on different forms because each shape has its own challenges. Also, every artist does things a little differently and you can always learn from getting multiple perspectives. I hope this will get you thinking about other forms to tackle with bisque stamps. -Jennifer Poellot Harnetty, editor
The jar and pitcher shown were made using this stamping process. Lisa chose glazing and firing treatments that would enhance the stamped textures on the pots and the looseness of the forms. When trying this process, be sure to consider your glazing and firing techniques with these things in mind. If you test this or Mark Peters’ stamped rim platter technique (or any other method you learned from a Ceramic Arts Daily feature), snap a photo of your finished and fired piece, and email it to the editor. It may be used in a future follow-up feature!
Lisa Bare Culp is an Ohio native and holds a bachelor’s degree in Fine Arts/Ceramics from the Columbus College of Art and Design. She has been teaching ceramics for more than ten years, most of which have been in her home studio, Bareclay. Bareclay Studio specializes in Lisa’s artwork, ceramic education and ceramic restoration/repair. Visit www.bareclay.com for more information and images.
Search the Daily
Published Jul 2, 2008
Lisa Bare Culp demonstrates a similar technique to Mark’s stamped rim technique, but on a simple vase form. I think it can valuable to see similar techniques on different forms because each shape has its own challenges. Also, every artist does things a little differently and you can always learn from getting multiple perspectives. I hope this will get you thinking about other forms to tackle with bisque stamps. -Jennifer Poellot Harnetty, editor
The jar and pitcher shown were made using this stamping process. Lisa chose glazing and firing treatments that would enhance the stamped textures on the pots and the looseness of the forms. When trying this process, be sure to consider your glazing and firing techniques with these things in mind. If you test this or Mark Peters’ stamped rim platter technique (or any other method you learned from a Ceramic Arts Daily feature), snap a photo of your finished and fired piece, and email it to the editor. It may be used in a future follow-up feature!
Lisa Bare Culp is an Ohio native and holds a bachelor’s degree in Fine Arts/Ceramics from the Columbus College of Art and Design. She has been teaching ceramics for more than ten years, most of which have been in her home studio, Bareclay. Bareclay Studio specializes in Lisa’s artwork, ceramic education and ceramic restoration/repair. Visit www.bareclay.com for more information and images.
**First published in 2008.
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques