Creative kiln loading is key to achieving unique soda-fired pottery surfaces. Thoughtful pot placement, stacking, and wadding can help guide flame and soda, creating beautiful flashing and distinctive marks.

 

Loading the kiln is a fundamental part of firing with soda. I create dynamic effects on the pots with creative loading. I take an intuitive approach with the use of wadding and placement of the pots to encourage flashing and glaze patterns that are a unique record of that particular firing. Placing unglazed pots next to each other in direct contact yields a dry surface in those areas while allowing the soda to build up in the more exposed areas of the pots. 

Before I begin loading the work, I come up with a rough plan of placement and create clusters and stacks of pots to load together on a shelf (Figure A). I play with variations for each piece, considering what position or angle to wad it in. It should be noted that the placement of the wad can have a dramatic effect on the pot as wads leave markings and can direct and divert the flame’s path. This can and should be exploited and used as a decorative element to enhance the piece. 

 

A1 To prepare a plate for firing, apply glue where wads will be attached.A2 Press the wads into the glue.

A3 Flip the plate over and lightly press to stabilize on the wads.A4 To add a second plate to the stack, wad it in a similar fashion to the first plate. Then stack to leave a flashing mark and maximize kiln space.

A5 Add a cup to the stacked plates with wads. All pieces are wadded to ensure the pieces don’t become glazed to each other during the firing process. Each stacked piece will leave a mark on the piece below it.

A6 Kiln post, brick shim, bowl, and plate ready for wadding.A7 Invert a bowl on a post using a large ball of wadding.

A8 Use a brick shim with wads on top and bottom between a bowl and plate to provide separation during the firing process.

With this in mind, I take cues from the individual pots to determine how many wads to use and where to place them on the piece (Figure B). Cups and bowls tend to get three to five wads unless there is an element of a pot that would suggest a particular wad pattern. For example, if the pot has seven sides, I might use seven wads to follow the piece’s design. 

B1 Cup with ball of wadding. B2 Press the cup into the ball of wadding at an angle.

B3 Cup wadded and ready for the kiln. B4 Mug and tumbler arranged together to encourage flashing. The close proximity will discourage soda vapor from landing in shielded areas. This will leave marks that disrupt the surface design continuity and display evidence of the atmospheric firing process.

B5 Mug and tumbler arranged together to encourage flashing. The close proximity will discourage soda vapor from landing in shielded areas. This will leave marks that disrupt the surface design continuity and display evidence of the atmospheric firing process. B6 Build clusters of vessels, considering how the atmospheric effects will interact with each piece.

B7 Each piece is carefully arranged with shape and size considered to encourage flashing for deliberate results.

If a pot has no glaze, the options are wide open as to how the piece gets loaded in the kiln: I can wad the pot upside down on a post or place it at an angle on a large wad. Small bowls and cups can be placed in large bowls or on top of plates (Figure C). Stacks of various forms wadded together can create dynamic surfaces that highlight the range of surfaces achieved in the soda-firing process. 

C1 Plate with wads glued on awaiting loading. C2 Plate and bowl wadded and stacked. Wads are placed intentionally to elevate the bowl above the surface of the plate. This allows airspace between pieces, enabling soda vapor and flame to travel between the pieces.

C3 Fired plate with wad still in place. C4 Fired plate with wadding removed, illustrating mark making potential with wadding size and placement.

For a typical firing, I wad a selection of work beforehand and leave the rest unwadded with the intention of filling in open gaps or creating blocks by determining how a piece is wadded right before it is loaded. One of the beautiful things about low-fire soda is that wadding is not always needed between stacks of pots. I have discovered amazing results by dry stacking pots together, though this only works with slipped or raw clay surfaces. 

Because soda at these temperatures does not flux as much and accumulates less than at high-fire temperatures, dry stacking and butting pots right up against one another is possible. I have seen remarkable flash marks from dry stacking and use the technique in most of my firings. Wadding can also be used as a decorating device by placing wads in, on top of, or next to pots to create vapor blocks, which promote flashing and can create interesting and dynamic designs and markings. By experimenting and taking notes, a multiplicity of effects and surfaces can be achieved with the use of thoughtful loading and wadding strategies. 

the author Neil Celani contributed this excerpt to Justin Rothshank’s book, Low-Fire Soda, published by The American Ceramic Society and available in the Ceramic Arts Network Shop: mycan.ceramicartsnetwork.org/s/product-details?id=a1B3u000009udqwEAA. 

 

Previous December Issue Article                    Next December Issue Article

 

December 2026: Table of Contents


Must-Reads from Ceramics Monthly

Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Topics:
Click the cover image to return to the Table of Contents