If cookie cutters, stamps, molds, or rollers are sticking to your stoneware clay, a light coating of cooking spray can make a surprising difference. I’ve used PAM®, a kitchen pan coating, for over a decade as a simple release agent, and it consistently helps produce crisp impressions and clean edges without the frustration of tools sticking to the clay.
The key is applying the spray to the tool, not the clay. Spray a small amount into a bowl and dip cookie cutters or stamps directly, or lightly coat a paper towel and wipe down tools such as plastic, metal, glass, cookie cutters, stamps, molds, or rubber rollers. The goal is a thin, even film that is just enough to create a release barrier while preserving fine details. After several impressions, reapply as needed.
Avoid using cooking spray on plaster tools, as clay naturally releases from plaster and it will clog plaster pores. I also avoid applying it to surfaces that will later be joined by slipping and scoring, since any oil residue could affect adhesion. Compared to cornstarch or plastic wrap alternatives, I find cooking spray is cleaner, faster, less messy, and it burns off cleanly in the kiln. This simple studio trick saves time, reduces frustration, and helps maintain sharp surface detail.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.
Please enjoy this complimentary article for the month.
For unlimited access to Ceramics Monthly premium content, please subscribe.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.
Subscribe to Ceramics Monthly
If cookie cutters, stamps, molds, or rollers are sticking to your stoneware clay, a light coating of cooking spray can make a surprising difference. I’ve used PAM®, a kitchen pan coating, for over a decade as a simple release agent, and it consistently helps produce crisp impressions and clean edges without the frustration of tools sticking to the clay.
The key is applying the spray to the tool, not the clay. Spray a small amount into a bowl and dip cookie cutters or stamps directly, or lightly coat a paper towel and wipe down tools such as plastic, metal, glass, cookie cutters, stamps, molds, or rubber rollers. The goal is a thin, even film that is just enough to create a release barrier while preserving fine details. After several impressions, reapply as needed.
Avoid using cooking spray on plaster tools, as clay naturally releases from plaster and it will clog plaster pores. I also avoid applying it to surfaces that will later be joined by slipping and scoring, since any oil residue could affect adhesion. Compared to cornstarch or plastic wrap alternatives, I find cooking spray is cleaner, faster, less messy, and it burns off cleanly in the kiln. This simple studio trick saves time, reduces frustration, and helps maintain sharp surface detail.
For more tips, follow Lescoe on Instagram @PotteryBySarah23.
December 2026: Table of Contents
Must-Reads from Ceramics Monthly
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Click the cover image to return to the Table of Contents