When an exciting but massive opportunity to make custom dinnerware for a local restaurant popped up, Suzanne Howard got organized and got to work in the studio. 

During a studio sale in May 2025, I noticed an unassuming, friendly guy checking out my wares. We got to talking, and he said he “needed some plates” for a restaurant he planned to open. He took my card and, much to my surprise, contacted me that same evening. After some Google sleuthing, I realized that the guy in question was Michelin-starred chef Jared Wentworth, who was opening Cafe Vivant in Menlo Park, California, and he needed nearly 300 dishes in six weeks. We met up soon after that, and he selected several patterns from my existing stock, giving me instructions on final sizes and color ideas. 

1 The first night the restaurant used Howard’s dishware she felt proud, delighted, and relieved. Also, very tired.

Into the Unknown 

As a dedicated hobbyist, this was a huge leap into the unknown land of the production potter. I was well-versed in making functional wares, even sets of plates for my own personal use–but never at this scale and speed. I had no storage space, no kiln of my own. 

I allowed myself a brief panic attack, then took a few deep breaths. Deep down, I knew I could do it—but how? I immediately enlisted the help of my amazing pottery community: Natalie and Vince, who generously offered me kiln and storage space; Margaret, owner of the studio where all wares were made; and Jee, who walked me through the production process for restaurant wares. I also got organized, which is not my strong suit. 

First stop: the Old Forge website (www.oldforgecreations.co.uk), which features a blog with incredible resources, including a pricing framework. I photographed, measured, and figured out costs for each sample, then created an invoice, ensuring that Jared reviewed and approved the specs. While waiting for the initial 50% upfront payment (and anxiously chomping at the bit to get started), I reviewed the work ahead, identifying potential pain points and brainstorming solutions. I identified which items would take the longest, and which therefore needed to be a priority. I made several bisque molds to save time down the road. I revisited how each sample pot had been made, sometimes recreating a pattern up to ten times before settling on the final technique. I researched glazes for Chef Jared’s approval. All this before throwing even a single pot! Perhaps most importantly, I created a Google Sheets calendar with every detail I needed to think about: daily/weekly schedule, clay pricing, glaze ideas and tests, and notes. I still use this document, and it has since expanded to reflect what’s going on in my pottery world, with details for upcoming events/sales, ideas to try, and resources to look into. 

In the early days of the project, I divided each day into morning (9 am–4 pm) and evening (7–10 pm) shifts. Between each shift, I’d nap, eat dinner, and walk the dog. At the end of each day, I’d review my trusty Google Sheet and prepare myself for what the next day would bring. I even created a nerdy macro to calculate the percentage of total wares I’d made. Tracking that number gave me a little daily boost, which brings me to the beauty of the community studio. 

2 Chef Jared Wentworth selecting patterns and dishes for production in the planning stage. 3 Peek into the storage closet midway through the project.

Space and Community 

Clay Creations, located in Pacifica, California, where this work was completed, is a bright, bustling space with people coming and going at all hours. Often, I’d arrive at the studio with the intention of glazing some wares, only to find the glaze room full or a glaze bucket in need of a refill. I then had to be adaptable and shift focus—trimming that day rather than glazing, for instance. Sometimes I’d do handbuilding work on the wheel because that was the only space available. Completing a large production in a community studio was not only an exercise in adaptability, but also highly gratifying. Word got around about the project, and many people would ask how it was going and offer their support and encouragement. Beautiful! 

All wares were made and stored at the studio in Pacifica until they reached the leather-hard stage, at which point I (very carefully) loaded them onto wareboards in my car and drove them around the curvy coastal cliffs and up and down the hills to my friend Natalie’s house, where they sat to fully dry and eventually get bisque fired. That was some of the slowest, safest driving of my entire life. Once bisque fired, I transported the wares back to the studio for glazing, then drove them to my friend Vince’s house to be glaze fired. This process repeated again and again. All glazed wares were stored in a large closet in a fourth location in Half Moon Bay. 

4 Oval plates in the greenware stage. 5 Various states of completion made it challenging to track inventory.

Problem Solving 

There were a few things I learned along the way. First, there are several key phases in this process. Getting near to “100% made” status—on which I’d been razor focused—meant there was still a mountain of bisque firing, glazing, refiring, and grinding work ahead. 

This would have been daunting if I had the time to think about it too much. I hovered at about “96% made” for many agonizing days as I re-made wares that had exploded in the bisque or whose glaze crawled. Problem-solving was a continual part of my process. I kept studious notes about each dish—amount and type of clay required, glazes, and measurements—and wore a tape measure around my neck like a seamstress. It also helped to have an easygoing chef: Jared was incredibly responsive and collaborative. He loved getting my updates with photos and “percentages made.” 

6 To keep studio tasks on track for the completion deadline, Howard made a schedule using Google Sheets.

When he sent me test photos of his food on the sample plates I’d provided him, things seemed to get real in the very best way. His work was (is) food art and my dishes were his canvas. When he ordered a second, smaller set of wares for his tasting menu, the initial 6-week experience gave me the confidence to stretch my wings and do more finessed work. For instance, trimming a subtle double lip on a plate to help frame the food and forming the base of a pinched bowl in a mold formed from a crystal platter . . . details that only the most eagle-eyed diner might see, but that the chef and dishwasher might notice and appreciate over time and use. When Jared came to pick up all the final dishes and bring them to the restaurant, he looked at the bursting closet and said, “You’ve been working very hard.” Yes Chef! 

7 When in use, these bespoke wares beautifully elevated Chef Jared Wentworth’s artfully prepared meal. Photo: Jim Sullivan.

A Satisfying End 

When at last the project was complete and the restaurant opened its doors, I was delighted to attend the friends-and-family soft opening. Though I was inexplicably nervous, it was deeply satisfying to see my wares showcasing Jared’s artistic culinary creations. It’s been an incredible rush to see my work highlighted on the restaurant’s social media and in reviews from Wine Spectator and Modern Luxury. Looking back, I sometimes miss that time period. It was all worth it, including my raw hands from throwing countless pounds of clay, and feeling like Cinderella as studio members went about their normal lives while I lived at the studio, day after day (I did take one day off). I do not even regret the time I spent staring up at the ceiling at night, worrying about the absurd possibility of an earthquake or a tidal wave taking out my entire stock in one fell swoop. It was not always rational or pretty, but I’d gladly do it all again. 

the author Suzanne Howard started her clay journey in 2015. The feeling of clay under her hands on the wheel hooked her for life, and she’s been enjoying every aspect of the medium since that fateful evening. She lives with her family and sweet dog on the stunning coast near San Francisco, California. 

 

Previous December Issue Article                    Next December Issue Article

 

December 2026: Table of Contents


Must-Reads from Ceramics Monthly

Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Click the cover image to return to the Table of Contents