One potter, passionate about sustainability, shares how responsibly grown wood, efficient kilns, shorter firings, and a homemade water scrubber can make wood firing greener.
Is there such a thing as “green” wood firing? Trees grow using carbon from the atmosphere, and when burned, that carbon returns to the air it came from. No new carbon is introduced to the atmosphere—that’s a positive! But what about the fine carcinogenic particulates created during wood combustion?
I have spent the past 55 years working as a potter, with most of that time involved in green issues related to my potting career. I describe myself as an “environmentally conscious potter” for want of a better term. This is how I perceive the world and interact with it. So, in that regard, I have been trying to live a sustainable life—well, as much as is possible, without becoming a bore.
Keeping Wood Sustainable
I used to fire with LPGas—everybody did in the 70s—but phased it out about a decade ago. Now I fire with electricity from our solar panels and batteries, or with self-grown wood from our own forest. We can fire with sunshine all year round, but it isn’t safe to fire with wood in the heat of summer, so we only fire with our homegrown forest timber in the winter.
My most recent research has been into how I can minimize the smoke and particulates coming from my wood-fired kiln chimney. I have developed a reasonably “clean” firing wood kiln by using a Bourry box downdraft firebox design. This kind of firebox minimizes smoke pollution, while still creating strong reducing conditions inside the chamber. I also keep my firings short, at around fourteen hours, to minimize particulates.
I wrote a book, Laid Back Wood Firing, all about this approach to wood firing. It is now in its 46th year of continuous publication, its 10th edition, and is available is French and Korean translations.
Wood can be a sustainable fuel if harvested thoughtfully and carefully. It is also almost carbon neutral. These are all great attributes. So I’m pleased to use our own homegrown wood as fuel for our house and pottery.
Wood fuel is only sustainable if it is harvested from vigorously growing forests. Felling trees to clear land for agriculture is not sustainable or green. We have nurtured our seven-acre bushland block in the Southern Highlands since 1976. We selectively take out dead, dying, or inconveniently placed trees, many of which we actually planted ourselves, but placed too close to buildings and fence lines in our naive, youthful enthusiasm. After 50 years of selective harvesting and careful management, there is a lot more carbon sequestered in our forest now than there was when we bought the mostly cleared block, back in 1976.
If I continue with my forest stewardship, we will probably have wood fuel for our home and kilns indefinitely. Given these circumstances, wood fuel will be part of our personal energy mix for the rest of my life.
Minimizing Micro-Particulates
So, this brings me to my recent interest in minimizing the particulates from my chimney. One way is to fire very quickly. I have been building small portable wood-fired kilns that fire to stoneware temperatures in reduction in three hours using just two wheelbarrow loads of wood! This reduces the amount of wood fuel burned, and therefore reduces the number of particulates released. Not the best solution, but a very good one, as it has several benefits combined in one project.
There have been a few articles in the environmental press in recent years about the harm resulting from micro-particulates, known as PM2.5 particulates. These are commonly found in diesel exhaust fumes, but also from un-flued gas heaters and gas kitchen cooktops.
I fire most of the time with a very clean chimney, with only occasional bursts of flame and/or smoke when a big log drops off the hob. However, after reading about these micro-particulates from other fuels that appear to be visually clean but are not, like gas stoves. It got me thinking that I should do something about the PM2.5 particulates that must be being emitted from my visually clean chimney top throughout the kiln firing.
Adding a Scrubber
My solution has been to incorporate a combined afterburner/ spark arrestor/scrubber on top of my chimney. There are two poly pipes connected. One takes the clean water up, the other takes the dirty water back down to be filtered and recycled. You can see there is a flame entering at the bottom and cleaned flue gases leaving at the top.
So far, the main issues that I can think of that need to be juggled to get a good outcome are:
Design of the spray
Pressure of the water
Size of the water droplets
Angle of the mist
Type of pump
Number of sprays
Filter
There may be others that I have not thought of yet. The unknown unknowns! The current model that I have on top of my chimney is a prototype. It works, but not as completely as I’d like. There is much more work to be done. I have ideas for an improved version in the works. However, this year I have been working on using different spray jets and various pressures to see what seems to work best.
Using Water
If the droplets are too big, they don’t have the surface area to interact with all the smoke/particles. If the droplets are too fine, they have good interaction, but are so small that they might evaporate into steam with the heat and carry the fine particulates away untrapped, dry out, and then fall back to earth for me to breathe.
The trick is to judge the size and distribution of the water droplets to find the sweet spot. This involves the combination of the design of the spray, the size of the orifice, the pressure of the water, and the shape of the mist. I thought that a very wide-angle, hollow-cone spray might work best, so that all the flue gases have to pass through the water mist.
I decided to use a submersible water pump for my initial experiments. This worked well, and seemed to give enough pressure to activate the spray jet up on top of the roof. A cheap Chinese-made submersible pump appeared to manage this okay. I started with just one spray jet, but later added another one above to create a two-tiered effect, to provide more surface area of droplets for the smoke to pass through.
I experimented with several options, but the brass garden sprinklers were as good as any, and with no moving parts. I bought several and experimented with them. I ended up testing three different sprinklers that produced a hollow-cone spray of droplets that would fill my scrubber. The flat brass hex-head one produced the widest, flattest, hollow-cone spray.
Filtering
I have tried different water filter designs. The most expensive one, which required an expensive replacement cartridge, is possibly the best choice for the job in terms of filtration. Initially, I thought I only needed a filter to remove particles large enough to block the spray jet. However, I came to realize that I need to remove the sub-micron particles entirely from the water system, so that they don’t get the chance to evaporate into the atmosphere on any subsequent trip around the system as the water is recycled.
I don’t suppose that this project will ever be finished to my satisfaction. I’ll keep tinkering with it as long as I’m wood firing and can still climb ladders onto rooftops. However, with just three to six wood firings a year in my kiln, it will take a long time to get a definitive answer—if ever.
Not using a recirculating pump, but instead using a one-pass, total-loss water system would be safest, but the most costly in terms of water usage. We live out in the bush, on rainwater harvested and stored in water tanks for our water supply. Therefore, water efficiency is important to me, so I haven’t pursued this total-loss option as of yet, but I think that it would be the best way to go if you have municipal water access. This would mean that you could eliminate the filter.
Work in Progress
What I have built and tested so far is adequate, but I see it as a work in progress, and by putting the concept out there for other like-minded potters to see and think about, perhaps someone else will come up with a better, improved solution that we can all learn from.
I can see a time coming in the future when coal-fired power stations are retired, and diesel and petrol cars are all replaced with electric versions. At that time, wood firing won’t be allowed unless you have a functioning scrubber or similar apparatus to clean up your solid-fuel appliance. If we develop and share our ideas and research now, when the time comes, we will be prepared and there is a chance we can continue firing our kilns, which would comply with any new “clean air” regulations.
Conclusions
The decision to use a 200-liter water tank reservoir was a good one for me. It allows me to see the extent of the discoloration of the water, this indicates some degree of efficiency. The water is completely black by the time the firing is over. The big advantage is that it allows me to recycle the water.
Blackness is certainly carbon, but not necessarily PM2.5-sized particulates. I don’t have the facilities to measure the size of the particles that I am removing from my chimney, but I just assume that there will be some collection of the fine particulates along with the coarser carbon.
The scrubber does reduce the amount of black smoke from the chimney and completely hides the flames at the chimney top, so neighbors cannot see them. No one is likely to call the fire brigade out if there are no flames to be seen and very little, if any, smoke.
I hope that someone else will take this project up from where I leave off and make a better job of it. I have one more thing to add! The cleanest firing is done using electricity generated from solar PV panels, backed up by a battery. Consider this as a possibility for your next kiln. If that’s not an option, a $450 material investment (plus your labor and time) to make your own scrubber may be the way to go.
the author Steve Harrison is an artist/potter, author, researcher, and post-modern peasant living in Australia, making wood-fired and solar-fired, self-made stoneware from local materials and single-stone porcelain. He has a PhD in ceramic materials, specializing in sericite porcelain. Please feel free to contact Harrison for design drawings and parts info at steve.cone10@gmail.com.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.
Please enjoy this complimentary article for the month.
For unlimited access to Ceramics Monthly premium content, please subscribe.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.
Subscribe to Ceramics Monthly
One potter, passionate about sustainability, shares how responsibly grown wood, efficient kilns, shorter firings, and a homemade water scrubber can make wood firing greener.
Is there such a thing as “green” wood firing? Trees grow using carbon from the atmosphere, and when burned, that carbon returns to the air it came from. No new carbon is introduced to the atmosphere—that’s a positive! But what about the fine carcinogenic particulates created during wood combustion?
I have spent the past 55 years working as a potter, with most of that time involved in green issues related to my potting career. I describe myself as an “environmentally conscious potter” for want of a better term. This is how I perceive the world and interact with it. So, in that regard, I have been trying to live a sustainable life—well, as much as is possible, without becoming a bore.
Keeping Wood Sustainable
I used to fire with LPGas—everybody did in the 70s—but phased it out about a decade ago. Now I fire with electricity from our solar panels and batteries, or with self-grown wood from our own forest. We can fire with sunshine all year round, but it isn’t safe to fire with wood in the heat of summer, so we only fire with our homegrown forest timber in the winter.
My most recent research has been into how I can minimize the smoke and particulates coming from my wood-fired kiln chimney. I have developed a reasonably “clean” firing wood kiln by using a Bourry box downdraft firebox design. This kind of firebox minimizes smoke pollution, while still creating strong reducing conditions inside the chamber. I also keep my firings short, at around fourteen hours, to minimize particulates.
I wrote a book, Laid Back Wood Firing, all about this approach to wood firing. It is now in its 46th year of continuous publication, its 10th edition, and is available is French and Korean translations.
Wood can be a sustainable fuel if harvested thoughtfully and carefully. It is also almost carbon neutral. These are all great attributes. So I’m pleased to use our own homegrown wood as fuel for our house and pottery.
Wood fuel is only sustainable if it is harvested from vigorously growing forests. Felling trees to clear land for agriculture is not sustainable or green. We have nurtured our seven-acre bushland block in the Southern Highlands since 1976. We selectively take out dead, dying, or inconveniently placed trees, many of which we actually planted ourselves, but placed too close to buildings and fence lines in our naive, youthful enthusiasm. After 50 years of selective harvesting and careful management, there is a lot more carbon sequestered in our forest now than there was when we bought the mostly cleared block, back in 1976.
If I continue with my forest stewardship, we will probably have wood fuel for our home and kilns indefinitely. Given these circumstances, wood fuel will be part of our personal energy mix for the rest of my life.
Minimizing Micro-Particulates
So, this brings me to my recent interest in minimizing the particulates from my chimney. One way is to fire very quickly. I have been building small portable wood-fired kilns that fire to stoneware temperatures in reduction in three hours using just two wheelbarrow loads of wood! This reduces the amount of wood fuel burned, and therefore reduces the number of particulates released. Not the best solution, but a very good one, as it has several benefits combined in one project.
There have been a few articles in the environmental press in recent years about the harm resulting from micro-particulates, known as PM2.5 particulates. These are commonly found in diesel exhaust fumes, but also from un-flued gas heaters and gas kitchen cooktops.
I fire most of the time with a very clean chimney, with only occasional bursts of flame and/or smoke when a big log drops off the hob. However, after reading about these micro-particulates from other fuels that appear to be visually clean but are not, like gas stoves. It got me thinking that I should do something about the PM2.5 particulates that must be being emitted from my visually clean chimney top throughout the kiln firing.
Adding a Scrubber
My solution has been to incorporate a combined afterburner/ spark arrestor/scrubber on top of my chimney. There are two poly pipes connected. One takes the clean water up, the other takes the dirty water back down to be filtered and recycled. You can see there is a flame entering at the bottom and cleaned flue gases leaving at the top.
So far, the main issues that I can think of that need to be juggled to get a good outcome are:
There may be others that I have not thought of yet. The unknown unknowns! The current model that I have on top of my chimney is a prototype. It works, but not as completely as I’d like. There is much more work to be done. I have ideas for an improved version in the works. However, this year I have been working on using different spray jets and various pressures to see what seems to work best.
Using Water
If the droplets are too big, they don’t have the surface area to interact with all the smoke/particles. If the droplets are too fine, they have good interaction, but are so small that they might evaporate into steam with the heat and carry the fine particulates away untrapped, dry out, and then fall back to earth for me to breathe.
The trick is to judge the size and distribution of the water droplets to find the sweet spot. This involves the combination of the design of the spray, the size of the orifice, the pressure of the water, and the shape of the mist. I thought that a very wide-angle, hollow-cone spray might work best, so that all the flue gases have to pass through the water mist.
I decided to use a submersible water pump for my initial experiments. This worked well, and seemed to give enough pressure to activate the spray jet up on top of the roof. A cheap Chinese-made submersible pump appeared to manage this okay. I started with just one spray jet, but later added another one above to create a two-tiered effect, to provide more surface area of droplets for the smoke to pass through.
I experimented with several options, but the brass garden sprinklers were as good as any, and with no moving parts. I bought several and experimented with them. I ended up testing three different sprinklers that produced a hollow-cone spray of droplets that would fill my scrubber. The flat brass hex-head one produced the widest, flattest, hollow-cone spray.
Filtering
I have tried different water filter designs. The most expensive one, which required an expensive replacement cartridge, is possibly the best choice for the job in terms of filtration. Initially, I thought I only needed a filter to remove particles large enough to block the spray jet. However, I came to realize that I need to remove the sub-micron particles entirely from the water system, so that they don’t get the chance to evaporate into the atmosphere on any subsequent trip around the system as the water is recycled.
I don’t suppose that this project will ever be finished to my satisfaction. I’ll keep tinkering with it as long as I’m wood firing and can still climb ladders onto rooftops. However, with just three to six wood firings a year in my kiln, it will take a long time to get a definitive answer—if ever.
Not using a recirculating pump, but instead using a one-pass, total-loss water system would be safest, but the most costly in terms of water usage. We live out in the bush, on rainwater harvested and stored in water tanks for our water supply. Therefore, water efficiency is important to me, so I haven’t pursued this total-loss option as of yet, but I think that it would be the best way to go if you have municipal water access. This would mean that you could eliminate the filter.
Work in Progress
What I have built and tested so far is adequate, but I see it as a work in progress, and by putting the concept out there for other like-minded potters to see and think about, perhaps someone else will come up with a better, improved solution that we can all learn from.
I can see a time coming in the future when coal-fired power stations are retired, and diesel and petrol cars are all replaced with electric versions. At that time, wood firing won’t be allowed unless you have a functioning scrubber or similar apparatus to clean up your solid-fuel appliance. If we develop and share our ideas and research now, when the time comes, we will be prepared and there is a chance we can continue firing our kilns, which would comply with any new “clean air” regulations.
Conclusions
The decision to use a 200-liter water tank reservoir was a good one for me. It allows me to see the extent of the discoloration of the water, this indicates some degree of efficiency. The water is completely black by the time the firing is over. The big advantage is that it allows me to recycle the water.
Blackness is certainly carbon, but not necessarily PM2.5-sized particulates. I don’t have the facilities to measure the size of the particles that I am removing from my chimney, but I just assume that there will be some collection of the fine particulates along with the coarser carbon.
The scrubber does reduce the amount of black smoke from the chimney and completely hides the flames at the chimney top, so neighbors cannot see them. No one is likely to call the fire brigade out if there are no flames to be seen and very little, if any, smoke.
I hope that someone else will take this project up from where I leave off and make a better job of it. I have one more thing to add! The cleanest firing is done using electricity generated from solar PV panels, backed up by a battery. Consider this as a possibility for your next kiln. If that’s not an option, a $450 material investment (plus your labor and time) to make your own scrubber may be the way to go.
the author Steve Harrison is an artist/potter, author, researcher, and post-modern peasant living in Australia, making wood-fired and solar-fired, self-made stoneware from local materials and single-stone porcelain. He has a PhD in ceramic materials, specializing in sericite porcelain. Please feel free to contact Harrison for design drawings and parts info at steve.cone10@gmail.com.
December 2026: Table of Contents
Must-Reads from Ceramics Monthly
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Click the cover image to return to the Table of Contents