In ceramics, a field grounded in long-standing tradition, meaningful innovation often begins with a simple question: what if? John Neely was driven by a creative curiosity that both honored the past and looked to the future, leading to a lasting legacy through the development of the train kiln.
After years of working in Japan with wood kilns and master potters, John Neely returned to the US in the 1990s to pursue a fundamental shift in kiln design. The structure he developed resembled a train, and the name “Train Kiln” soon followed as the design spread across the American ceramics landscape. Rooted in a respect for centuries of ceramic tradition and guided by his own curiosity, Neely’s design reconsidered how ash traveled through a kiln by using gravity to move ash downward rather than a draft moving it upward. This conceptual shift reshaped the relationship between fire, ash, and kiln architecture, resulting in the train kiln becoming one of the most influential designs in contemporary wood firing.
Following the death of John Neely in the summer of 2025, the importance of Neely’s contributions was greatly amplified, as his passing was mourned across the country and the world. At the time of his passing, graduate students at Syracuse University in New York were building a new train kiln, led by technician and former Neely student Austin Riddle. The kiln, named The Orange Blossom Special, stands as one of many examples within a broader lineage—one in which Neely’s ideas continue to circulate through teaching, mentorship, and the ongoing construction and firing of train kilns across the US.
Chance Favors the Prepared Mind
John Neely left for Japan in 1973 and spent ten years researching the effects of kiln atmospheres on clay bodies, as well as Japanese language, architecture, and food and drink culture. While in Japan, he worked with two types of wood kilns: anagama and Push-Me- Pull-You. Neely questioned the firing systems in these kilns. The anagama, designed with a downhill firebox, functions by moving the flame uphill through a big hole in the ground, forcing the ash to move upward. The Push-Me-Pull-You kiln requires the user to lie on the ground to stoke—an uncomfortable firing method. One of Neely’s most influential questions was deceptively simple: would it be easier to move ash downhill rather than uphill? By elevating the firebox and allowing gravity to assist the movement of ash through the kiln, Neely fundamentally altered how flame and particulates traveled across ware surfaces. This shift redirected ash paths and produced distinct surface effects that differed from those of traditional wood kilns. Another key feature of this kiln design is the step system at the lower front of the kiln, which allows air to enter the secondary air system to efficiently combust the coals at the bottom of the kiln. The train kiln not only changed the fuel distribution system, but it also produced a more efficient wood kiln.
Neely approached kiln building as an ongoing research practice. Early versions of the train kiln were adjusted, rebuilt, and refined through repeated firings. Each iteration offered new information about airflow, temperature variation, and ash distribution. Rather than seeking a finalized design, Neely embraced the kiln as an evolving system—one that could respond to different firing goals, materials, and communities.
The first iterations of the train kiln had a small throat and flue with a small, elevated firebox. This kiln design did not have enough room for fuel to combust. Subsequent kilns became wider, more rectangular, and less influenced by the anagama’s funnel-like shape. The original arch was changed to a cast throat arch, which resulted in a higher arch system.
The final iteration of the kiln came to Utah State University, when Neely received an internal grant. With the higher sprung arch, more rectangular, tubular shape, and the step system at the front of the kiln, the flame has the potential to move front to back unimpeded. The key to firing the kiln is simply controlling it with the load. Now, most train kilns are made with minuscule changes over time.
The Train Moves Across the World
The popularity of train kilns has grown exponentially in the US over recent years. Ted Neal, a student and colleague of Neely, is now known in his own right for his kiln-building abilities, traveling both inside and outside of the US to build kilns. He says, “The train is the most requested design.”
Although you can achieve wood-fired results through a variety of kilns, being able to fire a train kiln is a unique experience in its efficient use of resources, ability to be fired with a smaller crew, and the amount of control it allows in the firing process. The size of the kiln can vary, but its relatively compact scale allows for multiple firings throughout the year, making it an effective tool for sustained and iterative research. A smaller kiln also means smaller firing crews. While it requires at least two people to operate, a group of three or four creates a close, collaborative dynamic that encourages a strong sense of community.
As the kiln has traveled across the country and beyond, it has prompted new questions about how the design can be adapted and expanded. At Northern Arizona University, for example, a train kiln called The Switchback was developed to allow the direction of the fire to shift midway through the firing, encouraging wood ash to build up on multiple sides of the work.
More recently in Poland, Michal Puszczynski built a hybrid train kiln with a digitally controlled recirculating system. A large train kiln with an antechamber, basically behind the chimney, holds a high-temperature stainless steel heat exchanger with a triple damper. The dampers and controlled blower system push the heat from the chimney to the front of the kiln. As the train kiln continues to evolve, its growing popularity reflects not only its efficiency but its ability to adapt to new questions.
Legacy
As a teacher, artist, father, mentor, and more, Neely left behind a very strong legacy, with the train kiln being just one part. When speaking with some of his colleagues and students, it is clear that Neely saw potential in everyone and everything, and strived to make things the best they could be. From handcrafting tools for any niche activity and technique you could need, to leaving behind books to inspire students, to always being around the studio, Neely left a profound impression of care and a motivation to work hard, ask questions, and keep moving forward for those around him.
Like much in ceramics, the train kiln is not simply a tool but a lineage, passed from artist to artist through teaching, mentorship, and shared labor. Neely emphasized the responsibility that comes with using such a kiln, often entrusting students with his own work to be fired in their kilns. This gesture functioned as both encouragement and challenge, signaling belief in their abilities while reinforcing the kiln as a tool for careful research, discipline, and respect for the process.
Through these relationships, the train kiln moved across institutions and regions. Artists trained under Neely carried the design into their own teaching and studio practices, embedding it within academic settings. For example, Ted Neal, who worked as a technician alongside Neely at Utah State University, later constructed a train kiln at Ball State University in Indiana in 2007, shortly after beginning his position there. In this way, the kiln’s presence expanded through a network of educators and students, adapting to new contexts while maintaining its core principles.
At centers such as Fountain Square Clay Center in Indianapolis, Indiana, and Morean Clay Center in Tampa, Florida, these firings become sites where technical knowledge, social exchange, and creative practice converge, reinforcing the communal foundation of ceramic traditions. Designed to fire ceramic work for the table and hand, the train kiln’s size is well-suited for universities and community centers, offering a manageable yet dynamic wood-firing experience. More importantly, it fosters a culture of collective making. Train kilns require sustained, collaborative effort, bringing together groups of artists, students, and community members in the shared act of firing.
Following Neely’s death in 2025, this network of practice has taken on renewed meaning. At Syracuse University, The Orange Blossom Special has already been fired multiple times, standing not as a memorial but as an active continuation of his approach. In this way, Neely’s legacy remains embedded in use, carried forward through the communities that continue to build, fire, and evolve the train kiln.
the authors Danielle Chandler is a third-year MFA candidate at Syracuse University in the VPA program. She is originally from Collierville, Tennessee, and received her BA in studio art from Baylor University in 2023. Her work is centered around figurative ceramic sculpture.
Anna Witte is a ceramic artist and third-year MFA candidate at Syracuse University. Originally from Indiana, she earned her BA at the University of South Florida in Tampa in 2023.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.
Please enjoy this complimentary article for the month.
For unlimited access to Ceramics Monthly premium content, please subscribe.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.
Subscribe to Ceramics Monthly
The audio file for this article was produced by the Ceramic Arts Network staff and not read by the author.
In ceramics, a field grounded in long-standing tradition, meaningful innovation often begins with a simple question: what if? John Neely was driven by a creative curiosity that both honored the past and looked to the future, leading to a lasting legacy through the development of the train kiln.
After years of working in Japan with wood kilns and master potters, John Neely returned to the US in the 1990s to pursue a fundamental shift in kiln design. The structure he developed resembled a train, and the name “Train Kiln” soon followed as the design spread across the American ceramics landscape. Rooted in a respect for centuries of ceramic tradition and guided by his own curiosity, Neely’s design reconsidered how ash traveled through a kiln by using gravity to move ash downward rather than a draft moving it upward. This conceptual shift reshaped the relationship between fire, ash, and kiln architecture, resulting in the train kiln becoming one of the most influential designs in contemporary wood firing.
Following the death of John Neely in the summer of 2025, the importance of Neely’s contributions was greatly amplified, as his passing was mourned across the country and the world. At the time of his passing, graduate students at Syracuse University in New York were building a new train kiln, led by technician and former Neely student Austin Riddle. The kiln, named The Orange Blossom Special, stands as one of many examples within a broader lineage—one in which Neely’s ideas continue to circulate through teaching, mentorship, and the ongoing construction and firing of train kilns across the US.
Chance Favors the Prepared Mind
John Neely left for Japan in 1973 and spent ten years researching the effects of kiln atmospheres on clay bodies, as well as Japanese language, architecture, and food and drink culture. While in Japan, he worked with two types of wood kilns: anagama and Push-Me- Pull-You. Neely questioned the firing systems in these kilns. The anagama, designed with a downhill firebox, functions by moving the flame uphill through a big hole in the ground, forcing the ash to move upward. The Push-Me-Pull-You kiln requires the user to lie on the ground to stoke—an uncomfortable firing method. One of Neely’s most influential questions was deceptively simple: would it be easier to move ash downhill rather than uphill? By elevating the firebox and allowing gravity to assist the movement of ash through the kiln, Neely fundamentally altered how flame and particulates traveled across ware surfaces. This shift redirected ash paths and produced distinct surface effects that differed from those of traditional wood kilns. Another key feature of this kiln design is the step system at the lower front of the kiln, which allows air to enter the secondary air system to efficiently combust the coals at the bottom of the kiln. The train kiln not only changed the fuel distribution system, but it also produced a more efficient wood kiln.
Neely approached kiln building as an ongoing research practice. Early versions of the train kiln were adjusted, rebuilt, and refined through repeated firings. Each iteration offered new information about airflow, temperature variation, and ash distribution. Rather than seeking a finalized design, Neely embraced the kiln as an evolving system—one that could respond to different firing goals, materials, and communities.
The first iterations of the train kiln had a small throat and flue with a small, elevated firebox. This kiln design did not have enough room for fuel to combust. Subsequent kilns became wider, more rectangular, and less influenced by the anagama’s funnel-like shape. The original arch was changed to a cast throat arch, which resulted in a higher arch system.
The final iteration of the kiln came to Utah State University, when Neely received an internal grant. With the higher sprung arch, more rectangular, tubular shape, and the step system at the front of the kiln, the flame has the potential to move front to back unimpeded. The key to firing the kiln is simply controlling it with the load. Now, most train kilns are made with minuscule changes over time.
The Train Moves Across the World
The popularity of train kilns has grown exponentially in the US over recent years. Ted Neal, a student and colleague of Neely, is now known in his own right for his kiln-building abilities, traveling both inside and outside of the US to build kilns. He says, “The train is the most requested design.”
Although you can achieve wood-fired results through a variety of kilns, being able to fire a train kiln is a unique experience in its efficient use of resources, ability to be fired with a smaller crew, and the amount of control it allows in the firing process. The size of the kiln can vary, but its relatively compact scale allows for multiple firings throughout the year, making it an effective tool for sustained and iterative research. A smaller kiln also means smaller firing crews. While it requires at least two people to operate, a group of three or four creates a close, collaborative dynamic that encourages a strong sense of community.
As the kiln has traveled across the country and beyond, it has prompted new questions about how the design can be adapted and expanded. At Northern Arizona University, for example, a train kiln called The Switchback was developed to allow the direction of the fire to shift midway through the firing, encouraging wood ash to build up on multiple sides of the work.
More recently in Poland, Michal Puszczynski built a hybrid train kiln with a digitally controlled recirculating system. A large train kiln with an antechamber, basically behind the chimney, holds a high-temperature stainless steel heat exchanger with a triple damper. The dampers and controlled blower system push the heat from the chimney to the front of the kiln. As the train kiln continues to evolve, its growing popularity reflects not only its efficiency but its ability to adapt to new questions.
Legacy
As a teacher, artist, father, mentor, and more, Neely left behind a very strong legacy, with the train kiln being just one part. When speaking with some of his colleagues and students, it is clear that Neely saw potential in everyone and everything, and strived to make things the best they could be. From handcrafting tools for any niche activity and technique you could need, to leaving behind books to inspire students, to always being around the studio, Neely left a profound impression of care and a motivation to work hard, ask questions, and keep moving forward for those around him.
Like much in ceramics, the train kiln is not simply a tool but a lineage, passed from artist to artist through teaching, mentorship, and shared labor. Neely emphasized the responsibility that comes with using such a kiln, often entrusting students with his own work to be fired in their kilns. This gesture functioned as both encouragement and challenge, signaling belief in their abilities while reinforcing the kiln as a tool for careful research, discipline, and respect for the process.
Through these relationships, the train kiln moved across institutions and regions. Artists trained under Neely carried the design into their own teaching and studio practices, embedding it within academic settings. For example, Ted Neal, who worked as a technician alongside Neely at Utah State University, later constructed a train kiln at Ball State University in Indiana in 2007, shortly after beginning his position there. In this way, the kiln’s presence expanded through a network of educators and students, adapting to new contexts while maintaining its core principles.
At centers such as Fountain Square Clay Center in Indianapolis, Indiana, and Morean Clay Center in Tampa, Florida, these firings become sites where technical knowledge, social exchange, and creative practice converge, reinforcing the communal foundation of ceramic traditions. Designed to fire ceramic work for the table and hand, the train kiln’s size is well-suited for universities and community centers, offering a manageable yet dynamic wood-firing experience. More importantly, it fosters a culture of collective making. Train kilns require sustained, collaborative effort, bringing together groups of artists, students, and community members in the shared act of firing.
Following Neely’s death in 2025, this network of practice has taken on renewed meaning. At Syracuse University, The Orange Blossom Special has already been fired multiple times, standing not as a memorial but as an active continuation of his approach. In this way, Neely’s legacy remains embedded in use, carried forward through the communities that continue to build, fire, and evolve the train kiln.
the authors Danielle Chandler is a third-year MFA candidate at Syracuse University in the VPA program. She is originally from Collierville, Tennessee, and received her BA in studio art from Baylor University in 2023. Her work is centered around figurative ceramic sculpture.
Anna Witte is a ceramic artist and third-year MFA candidate at Syracuse University. Originally from Indiana, she earned her BA at the University of South Florida in Tampa in 2023.
December 2026: Table of Contents
Must-Reads from Ceramics Monthly
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Click the cover image to return to the Table of Contents