All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Alumina Hydrate 60.00
Kaolin 40.00
Wadding Recipe

Instructions

I use this high-alumina wadding recipe for porcelain fired in a soda kiln. 

Note: Use 60–70% alumina hydrate and 30–40% kaolin.

 