All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Water (in parts) 2.00
dried-red-clay-(in-parts) 1.00

Instructions

Add a small amount of Dolapix PC67 or any other deflocculant, just enough to thin the mixture. Allow the mixture to settle overnight before siphoning the usable terra sigillata. To make the red color deeper, add iron oxide.

 

This recipe was shared by Alexandra Nikolakopoulou in the March/April 2024 issue of Pottery Making Illustrated.