All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 31.00
Ferro Frit 3110 10.00
Alberta Slip 40.00
Ball Clay 19.00
Add Amount
cobalt carbonate 0.50
Copper Carbonate 3.00
Red Iron Oxide 1.00

Instructions

This recipe was shared by Michael Lemke in the May/June 2022 issue of Pottery Making Illustrated.