All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Goldart Bonding Clay 11.30
Fire Clay 10.87
Redart 7.39
Ball Clay 3.48
Silica 60.00
Potash Feldspar 3.48
Silica Sand 3.48

Instructions

Published in "Fire and Smoke" by George Sacco, in the Spring 2001 issue of Pottery Making Illustrated.