All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Talc 21.00
Whiting 12.00
Potash Feldspar 33.00
China Clay 15.00
Silica 16.00
Zinc Oxide 3.00
Add Amount
Nickel Oxide 3.00
Titanium Dioxide 10.00

Instructions

This recipe is from the November/December 2018 issue of Pottery Making Illustrated in the feature, "Developing Color: Yellow Glazes." This article is excerpted from Colour in Glazes by Linda Bloomfield.


This recipe is from the November/December 2018 issue of Pottery Making Illustrated in the feature, "Developing Color: Yellow Glazes." This article is excerpted from Colour in Glazes by Linda Bloomfield.