All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Dolomite 20.00
Nepheline Syenite 75.00
Ball Clay 5.00
Add Amount
Tin Oxide 5.00
Bentonite 2.00
Mason Stain Vanadium 6404 5.00

Instructions


*For Mellow Yellow, add Mason Stain Vanadium 6404, between 5–6%.

This is a white glaze that I modified to make it have a satiny surface.

This recipe was shared by Ashley Kim in the March/April 2019 issue of Pottery Making Illustrated.