All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Custer Feldspar 40.00
Whiting 20.00
Kaolin 10.00
Silica 30.00

Instructions

Published in "Woodfire Glazes" by Matt Schiemann, in the Jan 2014 issue of Ceramics Monthly.