All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Ball Clay 7.00
Cedar Heights Redart 86.00
Silica 7.00
Add Amount
Cobalt Carbonate 14.00
Copper Carbonate 14.00
Manganese Dioxide 64.00

Instructions

Published in "Modernist Series" in the Nov 2014 issue of Ceramics Monthly.
Fires to a metallic bronze. This glaze will brighten up if re-fired to cone 04. This glaze is not food safe.