All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Cornwall Stone 22.00
Soda Feldspar* 44.00
Whiting 18.00
Zinc Oxide 8.00
EPK Kaolin 3.00
Bentonite 5.00
Add Amount
Copper Carbonate 4.00
Titanium Dioxide 4.00

Instructions

The piece in the image shown here was glazed with Ashleigh's Rivulet and Frasca Ash (green) over Green Dragon Matte glaze.

Originally published in the Sept/Oct 2017 issue of Pottery Making Illustrated.
This glaze is a matte glaze and does not run if applied by itself. The glaze shown in the image above is a combination of Green Dragon Matte (applied first), Ashleigh's Rivulet, and Frasca Ash (green).

Warning: Ash glazes and the glaze combinations listed and shown above can and do run during the firing. Plan accordingly to protect your kiln and kiln shelves. Ian Hall-Hough side fires all of his pieces with runny glazes on seashells and wadding, which are then placed and fired on a drip tray (a waster slab that has been bisque fired and is used during the glaze firing to catch the glaze that runs off the pots). After the firing, Ian uses a rubbing stone and/or a Dremel to clean up any sharp edges shells to remove and leftover white powder (calcium oxide) that is left after the firing.