All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 15.00
Ferro Frit 3124 30.00
Custer Feldspar 45.00
Bentonite 10.00
Add Amount
Red Iron Oxide 35.00
Copper Carbonate 20.00
Cobalt Carbonate 12.00
Manganese Dioxide 5.00

Instructions

Smooth metallic sheen, similar to pencil lead. Will crawl when applied very thick.

Published in "Low-Fire Sculpture Glazes" by Holly Goring, in the December 2016 issue of Ceramics Monthly.