All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Bone Ash 7.08
Dolomite 14.16
Whiting 8.85
Custer Feldspar 44.25
Tin Oxide 4.42
EPK Kaolin 21.24
Add Amount
Red Iron Oxide 0.88
Rutile 0.88

Instructions

Matte glaze with a speckled tan color and a textured surface similar to fine sand.

Published in "Mid-Range Mattes" by Holly Goring, in the January 2017 issue of Ceramics Monthly.