All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 21.00
Potash Feldspar 27.00
China Clay 20.00
Silica 32.00
Add Amount
Yellow Stain (CdSZrSiO4) 4.00

Instructions

This recipe is from the November/December 2018 issue of Pottery Making Illustrated in the feature, "Developing Color: Yellow Glazes." This article is excerpted from Colour in Glazes by Linda Bloomfield.


This recipe is from the November/December 2018 issue of Pottery Making Illustrated in the feature, "Developing Color: Yellow Glazes." This article is excerpted from Colour in Glazesby Linda Bloomfield.