All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Bone Ash 25.00
Gerstley Borate 50.00
Nepheline Syenite 12.50
Copper Carbonate 12.50

Instructions

Published in "Tea and Friskets" by Frank James Fisher, in the Jul/Aug 2005 issue of Pottery Making Illustrated.