All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Grolleg 5.00
Water 4.00
Kona F4 3.00
Silica 2.00
Add Amount
Sodium Silicate 13.00
MS 6332 Orchid 25.00
MS 6376 50.00

Instructions

Published in "Layers of Color" by Andrews Gilliatt, in the Jan/Feb 2011 issue of Pottery Making Illustrated.


Note: 14 pounds of slip is just under one gallon. To make colored casting slip, add 100-120 grams (less for blue) of commercial stain per on gallon of slip, then ball mill the slip for at least two hours to ensure even dispersal of the colorant.