Glazes in which significant macrocrystalline structure forms in surface of low-alumina glaze seeded with zinc or titanium. Crystalline glazes feature large, visible crystal development, vs. microcrystalline effects, as in matt glazes and saturated-iron glazes. Source: Clay: A Studio Handbook