Copper Matt Raku Moloney Hi

You have read of of your complimentary recipes for the month.
For unlimited access to Ceramics Recipes premium content, please subscribe.
Yes, I want to subscribe to Ceramics RecipesWe understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.

You have read of of your complimentary recipes for the month.
For unlimited access to Ceramics Recipes premium content, please subscribe.
Yes, I want to subscribe to Ceramics RecipesNot right now. Continue to recipe.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.
Subscribe
Ingredients
Instructions
Remarkably, this versatile glaze is capable of producing a wide range of colors that are very receptive to atmospheric changes inside the kiln and outside in post reduction.
Published in "Fish Tales" by Lisa Merida-Paytes, in the Jul/Aug 2009 issue of Pottery Making Illustrated.
Through experimenting with the application of this glaze, I have been able to achieve a beautiful mottled surface with striking luster and opalescent color. I have found that applying less is better–one thin coat then wiping the glaze off with a dry towel works best to achieve a matte, speckled surface.
Recipe Topics
Clay Bodies and Casting Slips
Low Fire (Cone 022 – 01)
Mid Range (Cone 1 – 7)
High Fire (Cone 8 – 14)
Raku
Salt, Soda, and Wood
Slip, Engobe, and Terra Sigillata
Reference
Create your own Recipes!
You can keep your recipes private or share with others.
Create a Recipe
Manage your Recipes