Search the Daily

Published Oct 12, 2026

Drawing, Trailing, and Coloring: Creating Narrative Surfaces on Porcelain
Heidi McKay Casto's whimsical, storybook-style pots are truly an integration of form and surface. She combines throwing and handbuilding to make animals that seem to grow out of the pots! Then she brings them to life through a process of sketching, slip trailing with black underglaze, and filling in color like pages of a coloring book.

In this post, an excerpt from the September/October 2026 issue of Pottery Making Illustrated, Heidi walks through how she transfers her drawings onto bisqueware, how she fixes mistakes without damaging the surface, and more! –Jennifer Poellot Harnetty, editor

PS. To see how Heidi handbuilds her pots, check out the full article in the September/October 2026 issue of Pottery Making Illustrated. Not a subscriber? Subscribe today!


1 Bisque fire. Then, explore how to map out the drawings on each pot. 2 Draw the design on the pot with a cheap blue ballpoint pen.

Creating the Story 

In the days the pots are drying, I spend my time experimenting and exploring how to map out the drawings on each pot. I try to think through all the possibilities of what animals can take form on the surface, and how they might tell a story (1). 

Following the bisque firing, I sand each pot under water with 400-, 600-, and 800-grit wet/dry sandpaper to smooth the surface. 

3 Using a squeeze bottle, trace all the pen lines with black underglaze. 4 Add colorful designs, bisque fire again, apply a liner glaze before a final firing.

Images onto the Blank Canvases 

Using the story map in my sketchbook as a guide, I draw on the pot with a cheap blue ballpoint pen (2). The blue helps to provide contrast from the black underglaze I will use for slip trailing. I use a pen instead of a pencil to avoid graphite dust mixing with the underglaze, which I find occasionally creates bubbles in the underglaze after firing. 

If too much time has passed between drawing on the pot with a pen and applying the underglaze, I re-wet the pot before applying the underglaze so that it is cold to the touch. This tiny bit of hydration helps the pot not be so thirsty for the underglaze, making it easier to lay a solid, steady line. 

5 After the final firing, clean up any exposed porcelain with wet/dry sandpaper.

Using a squeeze bottle, I then trace all the pen lines with black underglaze (3). If I make a mistake, I wait until just after the underglaze dries enough to lose its sheen and carefully scrape away the mistake with a sharp knife at a 45-degree angle, being cautious only to remove the black line and not damage the pot. 

Once all the imagery has been outlined, I treat the piece like a coloring book, filling in the blank spaces with colorful designs. I continue to use glaze in squeeze bottles for this step (4). 

Heidi McKay Casto's Flaunt Your Fancy Feathers, porcelain, underglaze, glaze, fired in oxidation to cone 6.

Once I am satisfied with the design, I bisque the pots again. This vitrifies the design enough to stay put and burns out the pen marks, giving me a chance to see and fix the spots I may have missed. I put a liner glaze on the inside of the pots, leaving the outside free of any top glaze so the textures and details aren’t lost. 

Heidi McKay Casto's Sauntering Swans, porcelain, underglaze, glaze, fired in oxidation to cone 6. Beaches are for Lovers, porcelain, underglaze, glaze, fired in oxidation to cone 6.

Finishing Touches 

I do a final firing to cone 6 and then clean up any exposed porcelain with wet/dry sandpaper (5). When sanding, I first sand the bottom of my pots on the wheel with a 240-grit sanding bat, followed by 800-, 1000-, 1200-, 1500-, 2000-, 2500-, and 3000- grit wet/dry sandpaper, under water. 

Whether or not you use any of these skills in your own practice, I hope you take the time to exercise listening to your own instincts, especially in the studio. May your studio time be free of others’ expectations of what your work should be, allowing for more space for your unbiased creativity to take center stage. 

Heidi McKay Casto (she/her) is a ceramic artist and faculty member at The University of Iowa School of Art, Art History, and Design, where she is the Area Head of Ceramics. She earned her MA and MFA from the University of Iowa. Her work has been featured in over sixty group and four solo exhibitions. She was named a 2022 Ceramics Monthly Magazine Emerging Artist. 

Unfamiliar with any terms in this article? Browse our glossary of pottery terms!