Sometimes dipping your pots into a bucket of glaze isn’t an option, whether you are almost out of glaze, or you like to test a lot of pottery glazes and don’t mix up big batches to begin with. Sometimes you might not want a uniform dip of glaze for aesthetic reasons.
In today’s post, an excerpt from her videoLayering Techniques for Sumptuous Surfaces, Colleen Riley explains why her favorite way to glaze is with a ladle. Have a look and then add this method to your glaze application techniques repertoire! - Jennifer Poellot Harnetty, editor
PS. For some other great glaze application tips and techniques, check out this post!
Search the Daily
Published Jan 28, 2026
Sometimes dipping your pots into a bucket of glaze isn’t an option, whether you are almost out of glaze, or you like to test a lot of pottery glazes and don’t mix up big batches to begin with. Sometimes you might not want a uniform dip of glaze for aesthetic reasons.
In today’s post, an excerpt from her video Layering Techniques for Sumptuous Surfaces, Colleen Riley explains why her favorite way to glaze is with a ladle. Have a look and then add this method to your glaze application techniques repertoire! - Jennifer Poellot Harnetty, editor
PS. For some other great glaze application tips and techniques, check out this post!
This clip was excerpted from Layering Techniques for Sumptuous Surfaces, which is available in the Ceramic Arts Shop!
To learn more about Colleen Riley or to see more images of her work, please visit www.eurekapots.com/.
**First published in 2016.
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques