I fire to Cone 6 in my electric kiln and I am always on the lookout for great Cone 6 glaze recipes. It is so wonderful when you find glazes you adore. It’s even better when you can find two or more glazes you adore, AND that work well together!
In today’s post,Amelia Stamps shares two of the glazes she adores and her process for layering them to make them even more interesting! –Jennifer Poellot Harnetty, editor
Two Friendly Cone 6 Glaze Recipes
The Peacock jar shown here is decorated by overlapping the Chun glaze under the Chameleon glaze on a porcelain body. I decorate the bisqued piece by brushing on the Chun glaze in a dotted pattern. Sometimes I will use pencil on the bisque to lay out the pattern beforehand.
After the piece has the underneath pattern painted on I will then dip the entire piece in the Chameleon. No wax was used in my process. The combination of the glazes creates a pink halo effect around the Chun decoration that can resemble a peacock’s feather.
Chameleon is a Kathy Triplett glaze that I found in a glaze book years ago and the materials in the glaze have changed since then. Originally it called for “Nytal” Talc and “F-4” Felspar.
Now we are using Pioneer Talc and Minspar. It produces a similar result that is varied going from shiny green when thin and gray matte when thicker. (Example shown below) I use a white stoneware (BMix) and a grolleg porcelain. Glaze can go darker on the porcelain.
Search the Daily
Published Feb 20, 2018
In today’s post, Amelia Stamps shares two of the glazes she adores and her process for layering them to make them even more interesting! –Jennifer Poellot Harnetty, editor
The Peacock jar shown here is decorated by overlapping the Chun glaze under the Chameleon glaze on a porcelain body. I decorate the bisqued piece by brushing on the Chun glaze in a dotted pattern. Sometimes I will use pencil on the bisque to lay out the pattern beforehand.
After the piece has the underneath pattern painted on I will then dip the entire piece in the Chameleon. No wax was used in my process. The combination of the glazes creates a pink halo effect around the Chun decoration that can resemble a peacock’s feather.
Chameleon is a Kathy Triplett glaze that I found in a glaze book years ago and the materials in the glaze have changed since then. Originally it called for “Nytal” Talc and “F-4” Felspar.
Now we are using Pioneer Talc and Minspar. It produces a similar result that is varied going from shiny green when thin and gray matte when thicker. (Example shown below) I use a white stoneware (BMix) and a grolleg porcelain. Glaze can go darker on the porcelain.
**First published in 2016
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques