Published Mar 27, 2015
Slump molds are great for making plates since you can just drop the slab into the mold and not worry about it shrinking around it. They are even better when they are your own homemade mold.
In today's post, an excerpt from Platters: Four Approaches to Making and Decorating Plates, Ben Carter shares some tips on using an easy-to-make slump mold to make a large oval platter. –Jennifer Poellot Harnetty, editor
This clip was excerpted from Platters: Four Approaches to Making and Decorating Plates, which is available in the Ceramic Arts Network Shop!
To learn more about Ben Carter or to see more images of his work, please visit www.carterpottery.com.
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques
Search the Daily
Published Mar 27, 2015
In today's post, an excerpt from Platters: Four Approaches to Making and Decorating Plates, Ben Carter shares some tips on using an easy-to-make slump mold to make a large oval platter. –Jennifer Poellot Harnetty, editor
This clip was excerpted from Platters: Four Approaches to Making and Decorating Plates, which is available in the Ceramic Arts Network Shop!
To learn more about Ben Carter or to see more images of his work, please visit www.carterpottery.com.
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques