The handle on my Mike Jabbur coffee mug is one of my absolute favorites in my collection. The ear-shaped curve at the top of the handle is just perfect for my fingers to comfortably nestle into, and is now a shape I seek out in a handle…and something I have been incorporating into my own work.
Search the Daily
Published Jun 29, 2015
It's these details that make all of the difference. In today's clip, an excerpt from his DVD Precise Imprecision: Strengthening Throwing Skills to Create Dynamic Functional Pottery, Mike demonstrates his handle making process and discusses the details he considers to make them function well. – Jennifer Poellot Harnetty, editor
This clip was excerpted from Precise Imprecision: Strengthening Throwing Skills to Create Dynamic Functional Pottery, which is now available as a digital download or DVD in the Ceramic Arts Network Shop!
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques