Clay tools are a potter's best friend–especially homemade tools designed to be perfect for specific tasks. Just by doing some creative searching, it’s amazing how many useful tools can be gleaned from around the home.
As Debra Oliva explains in today's post, you can use everything from beads to discarded plastic-wrap boxes to create what you need exactly when you need it. - Jennifer Poellot Harnetty, editor
Once in a while an idea for a piece creates the need for a tool to perform a specific task. Since I am always anxious to get to the work, I want to find a tool quickly and get on with the best part, making the piece.
I begin by looking around at the bounty of household items, home hardware and tools, manufactured pottery tools, and so on to see if there is anything that might do the task after a quick modification. Often I find that I have to DIY my own pottery tools too.
More often than not, I find the perfect thing.
For etching clay surfaces, I needed a texture tool that could get into small spaces. The most obvious was to cut up serrated metal pottery ribs. That seemed a bit of a waste of a costly tool but it was easy and fast. While making dinner, my eyes fell upon the shiny, serrated metal strip on the box of a roll of plastic wrap. This solution is almost free and just as effective. I cut them into whatever size tool I need with a tin snip and insert them into an X-Acto blade handle. The serrated edges wear out over time but one strip of metal provides enough material to last quite a while. X-Acto blade handles can usually be found wherever office and craft supplies are sold. Tin snips are available in home supply stores and are an invaluable tool in my tool box.
The latest and greatest!
In addition to stunning images and inspirational stories, Ceramics Monthly delivers practical technical information to help you better understand ceramic art. With an eye on emerging talent, current trends, expert advice, and in-depth reviews, Ceramics Monthly is your number one source for the latest and greatest in ceramics.
For tiny impressions, I make stamping tools by gluing interesting bits, such as beads, to wooden handles saved from broken cut-off wires or pieces of a wooden dowel rod. I try to use pieces of wood that are only slightly larger than the item I am gluing to it so that I can position the stamp more precisely to impress the clay.
To create a double, (triple, quadruple, etc.) line tool, I use broken pin-tool tips, collected over time, or big needles. Rug needles work well as the tip may be a bit more rounded than sewing needles.
The quickest way to create a handle is from air-hardening pottery craft clay (found at craft stores). I space the pins as I like and push them into a coil of this clay, taking care to be sure they go in evenly. I don’t fuss with the handle. It doesn’t need to be pretty. I just want it to fit my hand comfortably and perform properly for my purposes.
I let it dry overnight and the tool is ready to use the next day. Should the pins fall out, they can be glued in with a strong adhesive. A handle can be made from scrap wood; however, that takes more effort and time than I want to spend.
Search the Daily
Published Nov 8, 2022
Clay tools are a potter's best friend–especially homemade tools designed to be perfect for specific tasks. Just by doing some creative searching, it’s amazing how many useful tools can be gleaned from around the home.
As Debra Oliva explains in today's post, you can use everything from beads to discarded plastic-wrap boxes to create what you need exactly when you need it. - Jennifer Poellot Harnetty, editor
Once in a while an idea for a piece creates the need for a tool to perform a specific task. Since I am always anxious to get to the work, I want to find a tool quickly and get on with the best part, making the piece.
I begin by looking around at the bounty of household items, home hardware and tools, manufactured pottery tools, and so on to see if there is anything that might do the task after a quick modification. Often I find that I have to DIY my own pottery tools too.
More often than not, I find the perfect thing.
For etching clay surfaces, I needed a texture tool that could get into small spaces. The most obvious was to cut up serrated metal pottery ribs. That seemed a bit of a waste of a costly tool but it was easy and fast. While making dinner, my eyes fell upon the shiny, serrated metal strip on the box of a roll of plastic wrap. This solution is almost free and just as effective. I cut them into whatever size tool I need with a tin snip and insert them into an X-Acto blade handle. The serrated edges wear out over time but one strip of metal provides enough material to last quite a while. X-Acto blade handles can usually be found wherever office and craft supplies are sold. Tin snips are available in home supply stores and are an invaluable tool in my tool box.
The latest and greatest!
In addition to stunning images and inspirational stories, Ceramics Monthly delivers practical technical information to help you better understand ceramic art. With an eye on emerging talent, current trends, expert advice, and in-depth reviews, Ceramics Monthly is your number one source for the latest and greatest in ceramics.
Check out a copy today!
For tiny impressions, I make stamping tools by gluing interesting bits, such as beads, to wooden handles saved from broken cut-off wires or pieces of a wooden dowel rod. I try to use pieces of wood that are only slightly larger than the item I am gluing to it so that I can position the stamp more precisely to impress the clay.
To create a double, (triple, quadruple, etc.) line tool, I use broken pin-tool tips, collected over time, or big needles. Rug needles work well as the tip may be a bit more rounded than sewing needles.
The quickest way to create a handle is from air-hardening pottery craft clay (found at craft stores). I space the pins as I like and push them into a coil of this clay, taking care to be sure they go in evenly. I don’t fuss with the handle. It doesn’t need to be pretty. I just want it to fit my hand comfortably and perform properly for my purposes.
I let it dry overnight and the tool is ready to use the next day. Should the pins fall out, they can be glued in with a strong adhesive. A handle can be made from scrap wood; however, that takes more effort and time than I want to spend.
**First published in 2015
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High Fire Glaze Recipes
Mid-Range Glaze Recipes
Low Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques