How to Throw a Large Porcelain Bowl Without Collapsing it
Whether you call it a large or medium bowl, Lorna gives you the tips to make this oversized bowl!
Lorna Meaden
No matter what Lorna Meaden says, I'd call the bowl she is throwing in this clip a large porcelain bowl, rather than a medium-sized bowl—especially since it is porcelain. But as she points out, it took 25 years to be able to call this bowl medium sized.
In this post, an excerpt from Lorna's video, Integrating Form and Surface with Porcelain, she demonstrates how to successfully throw large porcelain bowls. It might take some practice, but with these helpful tips, it will be easier than you think! - Jennifer Poellot Harnetty, editor
For most people who are new to throwing clay, an early goal is throwing large pots(that don’t weigh 40 pounds!). But it can be hard to figure out how to get
clay from the base up into the walls, as well as how to add shape without having the whole thing collapse. If you struggle with these problems, Martina Lantin shares three useful tips on throwing large pots to help you overcome obstacles
that might be holding you back!
Are you interested in creating large pots in sections? In this post, Andrew Buck explains Adrian King’s “warm throwing”
process for making a large vase on the potters wheel. If you have been wanting to learn how to throw large pots, this is an excellent tutorial.
Nic Collins is known for upsizing his pots. I liked what Nic had to say because it addressed some simple, but often overlooked, things to consider before you even put your clay on the wheel. Plus, it includes some great cross-section diagrams that clearly
show what should be happening both inside and outside of the pot. Follow these tips for throwing large pots and
you’ll soon be in charge of the clay!
Search the Daily
Published May 17, 2024
No matter what Lorna Meaden says, I'd call the bowl she is throwing in this clip a large porcelain bowl, rather than a medium-sized bowl—especially since it is porcelain. But as she points out, it took 25 years to be able to call this bowl medium sized.
In this post, an excerpt from Lorna's video, Integrating Form and Surface with Porcelain, she demonstrates how to successfully throw large porcelain bowls. It might take some practice, but with these helpful tips, it will be easier than you think! - Jennifer Poellot Harnetty, editor
This clip was excerpted from Integrating Form and Surface with Porcelain, which is available in the Ceramic Arts Network Shop!
Need more tips for throwing large?
For most people who are new to throwing clay, an early goal is throwing large pots(that don’t weigh 40 pounds!). But it can be hard to figure out how to get clay from the base up into the walls, as well as how to add shape without having the whole thing collapse. If you struggle with these problems, Martina Lantin shares three useful tips on throwing large pots to help you overcome obstacles that might be holding you back!
Are you interested in creating large pots in sections? In this post, Andrew Buck explains Adrian King’s “warm throwing” process for making a large vase on the potters wheel. If you have been wanting to learn how to throw large pots, this is an excellent tutorial.
Nic Collins is known for upsizing his pots. I liked what Nic had to say because it addressed some simple, but often overlooked, things to consider before you even put your clay on the wheel. Plus, it includes some great cross-section diagrams that clearly show what should be happening both inside and outside of the pot. Follow these tips for throwing large pots and you’ll soon be in charge of the clay!
**First published in 2012.
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High Fire Glaze Recipes
Mid-Range Glaze Recipes
Low Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques