We get a lot of requests for videos demonstrating how to make a teapot here at Ceramic Arts Daily, and it has always been a difficult request to fulfill because teapots are pretty involved little projects. But I finally found a teapot video that is about as succinct as they come—roughly 12 minutes (not bad, considering the process). And the great thing is, it doesn't sacrifice detail and good advice.
So, sit back and watch this excerpt from Stephen Jepson's Advanced Throwing Projects and Techniques. When you're done, you should have a darn good foundation for making your own little teapot. - Jennifer Poellot Harnetty, editor
Search the Daily
Published Jan 22, 2010
So, sit back and watch this excerpt from Stephen Jepson's Advanced Throwing Projects and Techniques. When you're done, you should have a darn good foundation for making your own little teapot. - Jennifer Poellot Harnetty, editor
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques